The influence of solution temperature on the microstructure and mechanical properties of TMW-4M3 superalloy has been investigated. Comparisons of mechanical properties have also been made between the heat-treated TMW-4M3 variants and the commercial U720Li. The key microstructural variables examined were grain size and the volume fraction and size of the strengthening gamma' precipitates that control the mechanical properties of these alloys. By increasing the solution temperature from 1373 K to 1393 K (1100 A degrees C to 1120 A degrees C), the volume fraction of primary gamma prime dropped from 16.9 pct to 14.5 pct, whereas the average grain size increased from 8.7 mu m to 10.6 mu m. Compared with an alloy with a smaller grain size, the alloy with a larger grain size exhibited superior resistances to creep and fatigue crack growth without the expense of reduced tensile strength and low-cycle fatigue resistance. This suggested that a higher solution temperature may benefit TMW-4M3 in terms of superior overall properties. The greater overall properties of TMW-4M3 variants than that of commercial U720Li were also demonstrated experimentally. The possible explanations for the improvement of mechanical properties were discussed.

参考文献

上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%