The effects of RE, V, Ti and B on the microstructure and properties of high chromium cast iron containing 3% molybdenum under as-cast and heat treatment conditions were investigated with the method of comparing experiments. The results show that with the increase of RE content, the primary austenite of high chromium east iron is obviously refined. The morphology of carbide is changed from netlike and lath to small multiangular isolated blocks or massive blocks, the isolated degree of carbide is improved obviously, and the size is significantly re-fined. The addition of V and B into high chromium cast iron can refine the microstructure, reduce coarse columnar crystals and make the carbide smaller and uniform. Through composite modification with RE, V, Ti and B, the hardness, wear resistance and impact toughness of high chromium cast iron are increased conspicuously. After heat treatment, the hardness of high chromium iron is increased significantly, but the toughness and wear resistance do not show great improvement.
参考文献
[1] | Zhang Y H;Wang G;Liu C C;Huang J.Z.Research and application of grinding balls of high chromium white cast iron with V Ti and RE[J].Heat Treat Met (in Chinese),1998(02):28. |
[2] | Hao S J.Wear Resistant High Chromium Cast Iron (in Chinese)[M].Coal Industry Press,Beijing,1993:162. |
[3] | Zhou Q D.Wear Resistance and Fracture Toughness of Chromium White Iron (in Chinese)[M].西安:西安交通大学出版社,1986:15. |
[4] | YangQingxiang,CuiZhanquan,LiaoBo,YaoMei.Effect of Rare Earth Elements on Growth Dynamics of Austenite in 60CrMnMo Steel[J].稀土学报(英文版),1999(01):46-48. |
[5] | Song Q;Meng F Q;Zhang H Y .The effect of heat treatment process on structure and properties of high chromium cast iron[J].Foundry (in Chinese),1998,9(04):44. |
[6] | Su Y L;Zhang X K;Zhang D Y;Kong L X,Xu J Q,and Zhao Y J .Strengthened principle of high chromium cast iron[J].Journal of Beijing University of technology,1991,17(03):58. |
[7] | Liu S P;Xu D;Sun K;Liu Y .Effects of vanadium and titanium on carbide morphology and wear resistance of high chromium cast iron[J].Hot Work Technol (in Chinese),2006,35(01):30. |
[8] | Wang J B;Li Q C .The effect of compound inoculation with rare earth on fatigue and wear behavior of high chromium cast iron[J].Journal of the Chinese Rare Earth Society,1994,12(03):279. |
[9] | He J A;Wang Y W;Liu G C;Tian D S,Cben Y H,and Tao J .Effect of rare earth treatment on wear resistant properties of low chromium cast iron[J].Chin Rare Earths (in Chinese),1991,12(06):18. |
[10] | Han F S;Pan X F;Zhang R;Zhang Z.Y.Improving the structure and the properties of low chromium white cast Iron by modification[J].Foundry (in Chinese),1990(01):1. |
[11] | 张宇彤,王丽萍.RE对高铬铸铁变质效果的研究[J].哈尔滨理工大学学报,2005(03):7-10. |
[12] | Guo E J;Wang L P;Yu Z J;Ma G R,and Fu Y K .Study on effects of rare earths and RE-Al modification treatment on high chromium cast iron[J].Journal of the Chinese Rare Earth Society,2005,23(02):214. |
[13] | Petrovic ST.;Markovic S.;Pavlovic ZA. .The effect of boron on the stereological characteristics of the structural phases present in the structure of the 13% Cr white iron[J].Journal of Materials Science,2003(15):3263-3268. |
[14] | Guan Y;Jin Z P .Study on the structure and properties of high chromium white cast iron and its tempering standard[J].Journal of Central South University of Technology(English Edition),1999,6(01):8. |
[15] | 马国睿,郭二军,王丽萍.稀土镁对高铬铸铁变质效果的研究[J].哈尔滨理工大学学报,2005(04):33-35,40. |
[16] | Liu G S;Wang W C .Study on the effect of Re and Al complex modification treatment on the structure and properties of high chromium alloy cast iron containing boron[J].J Hebei Univ Technol (in Chinese),1995,24(04):86. |
[17] | Zhi X H;Han Y J;Peng J Y .Study on effect of titanium on refinement of hypereutectic high chromium cast iron[J].Rare Met Mater Eng (in Chinese),2008,37(01):101. |
[18] | Randle V;Laird G .A microtexture study of eutectic carbides in white cast irons using electron back scatter diffraction[J].Journal of Materials Science,1993,28(15):4245. |