采用浸渍法制备了用于催化湿式氧化工艺的负载型CuO/γ-Al2 O3催化剂,采用XRD、FT-IR、SEM对其进行了表征,并以CN-为目标污染物,考察了CuO/γ-Al2 O3催化剂的催化活性和稳定性.试验研究表明:催化剂中的活性组分Cu是以CuO的形式存在,并且成功负载于载体γ-Al2 O3;对于初始质量浓度为2000 mg /L 的含氰废水,反应温度为130℃,搅拌速度为600 r/min,pH值为8,催化剂投加量为0.5 g/L,氧化剂30% H2 O2用量为5 mL/L废水时,反应时间30 min,CN-去除率可达到99%以上;重复使用30次后,催化活性大幅度降低.

@@@@CuO/γ-Al2 O3 catalyst was prepared by impregnation method .X-ray diffraction(XRD),Fourier trans-form infrared spectroscopy (FT -IR) and scanning and electron microscope ( SEM) techniques were performed to characterize CuO/γ-Al2 O3 catalyst.The catalytic activity and stability of the prepared catalyst was investigated by cata-lytic wet oxidation process of cyanide-containing wastewater.The results show that active component Cu was detected in the form of CuO and was successfully loaded on the carrier γ-Al2 O3 .The 99 % CN- removal efficiency of 2 000 mg/L cyanide-containing wastewater could be attained in 30 min with the parameters of temperature of 130℃, stirring speed of 600 r/min,pH value of 8,reagent dosage of 0.5 g/L CuO/γ-Al2 O3 and oxidant 30%H2 O2 dosage of 5 mL/L.The catalytic activity was significantly decreased after being reused 30 times.

参考文献

[1] 顾桂松,胡湖生,杨明德.含氰废水的处理技术最近进展[J].环境保护,2001(02):16-19.
[2] 郑道敏,方善伦,李嘉.含氰废水处理方法[J].无机盐工业,2002(04):16-18.
[3] 陈华进,李方实.含氰废水处理方法进展[J].江苏化工,2005(01):39-43.
[4] 薛文平,薛福德,姜莉莉,付瑞娟,褚亮亮,王晓霞,马洪杰.含氰废水处理方法的进展与评述[J].黄金,2008(04):45-50.
[5] 梁达文.含氰废水处理方法评价[J].玉林师范学院学报,2004(03):48-52.
[6] 吴超飞,王刚,杨波,吴海珍,任源,韦朝海.催化氧化法处理含甲醛毒性有机废水的工程试验[J].环境工程,2002(02):7-9.
[7] 安路阳,薛文平,马红超,马春,姜东.催化湿式氧化法处理高浓度含氰废水[J].大连工业大学学报,2012(03):199-202.
[8] An Luyang;Xue Wenping.Activity and Stability of Cu Catalyst in Cat-alytic Wet Air Oxidation of Cyanide-Containing Wastewater[A].北京:科学出版社,2011:914-921.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%