对三和金业生物氧化-氰化炭浸提金工艺进行了优化改造。通过优化生物氧化作业参数,使其处理能力提高了42.49 t/d;增设氧化洗涤液二段沉淀回收高品位含金微细氧化渣、采用二段沉淀-压滤工艺回收粉炭、增设摇床重选工艺回收氰渣中的金等,金的总回收率提高了0.46%。企业年增产黄金884.4 kg,取得了显著的经济效益。

Optimization of bio-oxidation-CIL after cyanidation process gold leaching process was carried out in Sanhe gold mining company .The processing capability was increased by 42 .49 t/d with the optimization of bio-oxida-tion operation parameters .Through adding a two-staged process for precipitating oxidation elution solution to recover high grade gold-containing micro fine oxidation residues ,applying two-staged precipitation-filter pressing process to re-cover carbon power and supplementing with a gravity separation process using tables to recover gold from cyanidation slags.Thanks to these measures , total recovery of gold was increased by 0.46 % and annual gold production by 884.4 kg,achieving notable economic benefits .

参考文献

[1] 吴学敏;杨凤 .江西三和金业有限公司金精矿及生物氧化渣金工艺性状研究鉴定报告[R].长春:长春黄金研究院,2009.
[2] 康国爱;陈发上.氰化尾渣回收金、硫试验研究与工业化实践[J].黄金,2010(增刊1):96-97.
[3] 王海东;张清波 .江西三和金业有限公司100吨/日生物氧化提金厂可行性研究报告[R].长春:长春黄金研究院,2004.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%