针对某含铜金矿石进行了氨氰法浸金及浸出贵液脱铜试验研究。其结果表明:在一定条件下,可获得较好的技术指标,浸渣金品位0.38 g/t,浸出贵液金、铜平均质量浓度分别为2.27 mg/L、61.94 mg/L,渣计金浸出率为89.44%;采用双氧水除铜,铜沉淀率为85.85%,氧化沉淀渣铜品位超过50%,可以铜精矿出售。

Gold extraction was studied from a gold ore with copper by ammonia cyanide leaching in the paper as well as copper removal from pregnant solutions .The leaching results showed that in certain conditions ,satisfactory tech-nical indexes could be obtained ,with leaching residues grade of 0.38 g/t,average mass concentration of gold and copper in leaching pregnant solutions respectively are 2.27 mg/L and 61.94 mg/L,gold leaching rate according to residues is 89.44 %.Hydrogen peroxide is used for copper removal ,gaining a copper precipitation rate of 85.85 %,and copper grade in the oxidation precipitation slags is over 50 %,making it possible to sell them as copper concentrates .

参考文献

[1] 曹昌琳.用氨-氰化物混合液从含铜金矿中选择性浸取金[J].黄金科技动态,1993(05):24-31.
[2] 夏光祥;涂桃枝;石伟 等.氨氰法从含铜金矿石中提金研究与工业实践[J].黄金,1995,16(07):26-29.
[3] 王宝胜,邓尧增,刘万志,谭丽萍.强化浸出降低氰化钠用量的试验研究和应用[J].黄金,2001(11):39-42.
[4] 张兴仁.氨-氰化物体系浸出铜 -金矿石的机理[J].国外黄金参考,1997(07):29-33.
[5] 殷芳喜.利用氧化铜矿石生产氧化铜的实践[J].矿产保护与利用,1998(01):34-36.
[6] 田国峰,赵蕾.含铜金矿石氨氰体系浸金机理研究[J].黑龙江科技信息,2010(12):18-19.
[7] 程东会,王金祥,李国斌,张晓燕,王立群.含铜金矿石氨氰体系浸金机理研究[J].有色金属(冶炼部分),2009(04):30-33.
[8] 王中溪,黄怀国,熊明,穆国红,蔡创开,陈景河.某含铜金矿石氨氰柱浸提金试验[J].黄金科学技术,2013(02):90-93.
[9] 程东会,李国斌,张晓燕,王立群,赵芳玲.含铜金精矿选择性浸金研究[J].黄金,2009(03):43-46.
[10] 涂桃枝,韩宝玲,黄成春,夏光祥.氨浸-氰化法处理含铜金精矿的研究[J].化工冶金,1989(04):38-43.
[11] 张云;李鸿雷 .硫代硫酸铵法从焙烧后的某含铜硫金精矿中回收金[J].黄金,1999,20(07):32-35.
[12] 方兆珩,Muhammed M.氰氨混合溶液浸取含铜硫化精矿中的金和银[J].中国有色金属学报,1992(01):39-45.
[13] 李敦钫.氨水对浸金氰化液离子平衡影响分析[J].昆明理工大学学报,2001(02):12-15.
[14] 张兴仁.氨 -氰化物混合溶液从铜 -金矿石中选择性浸出金[J].国外黄金参考,1994(02):26-31.
[15] 童雄,崔毅琦,黄宇林.某金矿氰化浸出液的树脂和活性炭吸附试验研究[J].有色金属(选矿部分),2005(02):9-12.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%