甘肃某细粒浸染型金矿石中金主要以包裹金形态存在,且载金矿物黄铁矿与脉石矿物连生关系复杂.针对该矿石的性质,进行了选矿试验研究.其结果表明:在最佳试验条件下,采用阶段磨矿-阶段浮选工艺,可获得金品位30.17 g/t、金回收率81.23%的较好指标;硫精矿经氧化焙烧—氰化浸出,金对原矿的回收率为6.96%,金总回收率达88.19%.
Mineral processing test was carried out for a fine grain disseminated gold ore from Gansu Province.The gold-carrying mineral is pyrite and it is connected with gangue minerals in a complex way.The test results under opti-mal test conditions,a stage grinding-stage flotation process can obtain a gold grade of 30.17 g/t and a gold recovery rate of 81.23 %.Sulfur concentrates go through roasting-cyanide leaching process,the recovery of primary gold ores is 6.96 %and the total recovery rate of gold is 88.19 %.
参考文献
[1] | 张立征;王彩霞;赵福财.甘肃某微细粒浸染型难处理金矿选矿试验研究[J].矿冶工程,2011(4):45-47. |
[2] | 郭玉武;张宇;朱恩领;魏党生;叶从新;韦华祖.内蒙古某微细粒浸染型金矿选矿工艺研究[J].有色金属(选矿部分),2015(4):46-50. |
[3] | 余世磊;王毓华;王进明;张英;余胜利.新疆某黄铁矿型低品位金矿石浮选试验[J].金属矿山,2013(5):78-81,91. |
[4] | 李艳军;陈波.山东某金矿石浮选试验[J].金属矿山,2013(7):91-92,96. |
[5] | 周中定.微细粒浸染型金矿石选金试验研究[J].黄金,2003(06):43-45. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%