热喷涂金属陶瓷涂层由于具有优异的耐磨性能,广泛应用于机械零部件的性能提升。热喷涂金属陶瓷涂层在复杂工况中服役时,在多种外界因素的复合作用下,会发生由磨粒磨损、腐蚀磨损、冲蚀磨损、疲劳磨损中的一种或几种作用导致的失效。结合涂层的服役工况和其自身结构特点归纳分析了热喷涂金属陶瓷涂层的复合磨损失效机制,并对热喷涂金属陶瓷涂层复合磨损失效研究的发展方向进行了展望。
Thermally sprayed cermet coating has been widely used in the improvement of mechanical compo-nents for its excellent wear resistance.Thermally sprayed cermet coatings suffer from abrasive wear,corrosion wear, erosion wear,and fatigue wear under the effect of complex external factors during service process.The composite wear failure mechanism of thermal sprayed cermet coating is analyzed based on the service condition and the micro-structure characteristics of the coatings.The development trend of the research on the wear failure of thermal sprayed cermet coatings is discussed as well.
参考文献
[1] | Brioua, S.;Belmokre, K.;Debout, V.;Jacquot, P.;Conforto, E.;Touzain, S.;Creus, J..Corrosion behavior in artificial seawater of thermal-sprayed WC-CoCr coatings on mild steel by electrochemical impedance spectroscopy[J].Journal of solid state electrochemistry,20122(2):633-648. |
[2] | 李松林;向锦涛;周伍喜;李玉玺;陈文.超音速火焰喷涂WC-10Co4Cr涂层的耐滑动磨损行为[J].中国有色金属学报(英文版),2012(5):1371-1376. |
[3] | Robert J.K.Wood.Tribology of thermal sprayed WC-Co coatings[J].International Journal of Refractory Metals & Hard Materials,20101(1):82-94. |
[4] | C. N. Machio;G. Akdogan;M. J. Witcomb;S. Luyckx.Performance of WC-VC-Co thermal spray coatings in abrasion and slurry erosion tests[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20051/4(1/4):434-442. |
[5] | Kanchan Kumari;K. Anand;Michelangelo Bellacci;Massimo Giannozzi.Effect of microstructure on abrasive wear behavior of thermally sprayed WC-10Co-4Cr coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,201011/12(11/12):1309-1319. |
[6] | Lalit Thakur;Navneet Arora.A comparative study on slurry and dry erosion behaviour of HVOF sprayed WC-CoCr coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20131/2(1/2):405-411. |
[7] | Hawthorne H.M.;Immarigeon J.P.;Legoux J.G.;Parameswaran V.R.;Arsenault B..Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,19992(2):825-834. |
[8] | M. R. Ramesh;S. Prakash;S. K. Nath;Pawan Kumar Sapra;B. Venkataraman.Solid particle erosion of HVOF sprayed WC-Co/NiCrFeSiB coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20103/4(3/4):197-205. |
[9] | Y. Y. Santana;J. G. La Barbera-Sosa;A. Bencomo.Influence of mechanical properties of tungsten carbide-cobalt thermal spray coatings on their solid particle erosion behaviour[J].Surface Engineering,20124(4):237-243. |
[10] | Study of erosion behaviour of conventional and nanostructured WC-12Co coatings sprayed by atmospheric plasma[J].Key engineering materials,2010:35. |
[11] | Jia-jie Kang;Bin-shi Xu;Hai-dou Wang;Cheng-biao Wang.Competing failure mechanism and life prediction of plasma sprayed composite ceramic coating in rolling-sliding contact condition[J].Tribology International,2014:128-137. |
[12] | Zhongyu Piao;Binshi Xu;Haidou Wang;Chunhuan Pu.Influence of undercoating on rolling contact fatigue performance of Fe-based coating[J].Tribology International,20101/2(1/2):252-258. |
[13] | X. C. Zhang;B. S. Xu;S. T. Tu;F. Z. Xuan;H. D. Wang;Y. X. Wu.Fatigue resistance and failure mechanisms of plasma-sprayed CrC-NiCr cermet coatings in rolling contact[J].International Journal of Fatigue,20095(5):906-915. |
[14] | R. Ahmed.Contact fatigue failure modes of HVOF coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20023/4(3/4):473-487. |
[15] | Stewart S;Ahmed R;Itsukaichi T.Rolling contact fatigue of post-treated WC-NiCrBSi thermal spray coatings[J].Surface & Coatings Technology,20052/3(2/3):171-189. |
[16] | Jia-jie Kang;Bin-shi Xu;Hai-dou Wang;Cheng-biao Wang.Influence of contact stress on rolling contact fatigue of composite ceramic coatings plasma sprayed on a steel roller[J].Tribology International,2014:47-56. |
[17] | 王海斗;张志强;李国禄;徐滨士;朴钟宇.等离子喷涂层接触疲劳失效模式及失效机理的研究[J].摩擦学学报,2012(3):251-257. |
[18] | M. R. Thakare;J. A. Wharton;R. J. K. Wood;C. Menger.Investigation of micro-scale abrasion-corrosion of WC-based sintered hardmetal and sprayed coating using in situ electrochemical current-noise measurements[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,200911(11):1967-1977. |
[19] | M. R. Thakare;J. A. Wharton;R. J. K. Wood;C. Menger.Exposure effects of strong alkaline conditions on the microscale abrasion-corrosion of D-gun sprayed WC-10Co-4Cr coating[J].Tribology International,20087(7):629-639. |
[20] | M. M. Stack;M. T. Mathew;C. Hodge.Micro-abrasion-corrosion interactions of Ni-Cr/WC based coatings: Approaches to construction of tribo-corrosion maps for the abrasion-corrosion synergism[J].Electrochimica Acta,201124(24):8249-8259. |
[21] | R. H. Shipway;L. Howell.Microscale abrasion-corrosion behaviour of WC-Co hardmetals and HVOF sprayed coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20051/4(1/4):303-312. |
[22] | M. A. Uusitalo;P. M. J. Vuoristo;T. A. Mantyla.Elevated temperature erosion-corrosion of thermal sprayed coatings in chlorine containing environments[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20027/8(7/8):586-594. |
[23] | J. F. Flores;A. Neville;N. Kapur;A. Gnanavelu.Erosion-corrosion degradation mechanisms of Fe-Cr-C and WC-Fe-Cr-C PTA overlays in concentrated slurries[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,200911(11):1811-1820. |
[24] | J. F. Flores;A. Neville;N. Kapur;A. Gnanavelu.An experimental study of the erosion-corrosion behavior of plasma transferred arc MMCs[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2009Pt.1(Pt.1):213-222. |
[25] | V. A. D. Souza;A. Neville.Aspects of microstructure on the synergy and overall material loss of thermal spray coatings in erosion-corrosion environments[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20071/6(1/6):339-346. |
[26] | Espallargas N;Berget J;Guilemany JM;Benedetti AV;Suegama PH.Cr3C2-NiCr and WC-Ni thermal spray coatings as alternatives to hard chromium for erosion-corrosion resistance[J].Surface & Coatings Technology,20088(8):1405-1417. |
[27] | J. F. Flores;A. Neville;N. Kapur;A. Gnanavelu.Corrosion and Erosion-Corrosion Processes of Metal-Matrix Composites in Slurry Conditions[J].Journal of Materials Engineering and Performance,20123(3):395-405. |
[28] | V. A. de Souza;A. Neville.Corrosion and erosion damage mechanisms during erosion-corrosion[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20031/6(1/6):146-156. |
[29] | G.C. Saha;T.I. Khan;G.A. Zhang.Erosion-corrosion resistance of microcrystalline and near-nanocrystalline WC-17Co high velocity oxy-fuel thermal spray coatings[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,20116(6):2106-2114. |
[30] | M. M. Stack;T. M. Abd El-Badia.Some comments on mapping the combined effects of slurry concentration, impact velocity and electrochemical potential on the erosion-corrosion of WC/Co-Cr coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,20089/10(9/10):826-837. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%