为细化WCoB-TiC-Co复相金属陶瓷晶粒,改善其组织,提高其力学性能,以WC、TiB2和Co粉末为主要原材料,采用真空液相原位反应烧结工艺,在1 400℃真空烧结炉中制备了WCoB-TiC-Co复相金属陶瓷.利用FE-SEM、EDS和XRD等技术,研究了不同含量的晶粒长大抑制剂VC对WCoB-TiC-Co复相金属陶瓷组织、物相构成、硬度、密度、耐磨性及抗弯强度和断口形貌等性能的影响.结果表明:添加适量的VC能有效细化WCoB-TiC-Co复相金属陶瓷晶粒,使得材料获得更均匀细小的微观组织,增加材料韧性和断口不平整性,增强材料抗弯强度,并且提高硬度、密度和耐磨性;当VC的质量分数增加到0.9%时,金属陶瓷的晶粒平均尺寸可细化到约1.3 μm,硬度随之升高到91.5 HRA,抗弯强度达到794 MPa;但VC的质量分数继续增加到1.2%、1.5%时,其硬度、密度、耐磨性及抗弯强度均会有所降低.
In order to refine the grain of WCoB-TiC-Co double phase cermet and improve its microstructure and mechanical properties,using WC,TiB2 and Co powders as main raw materials,WCoB-TiC-Co multiphase metal-ceramics were prepared by in-situ liquid-phase reaction sintering at 1 400 ℃ in the vacuum furnace.The effect of contents of VC grain growth inhibitor on microstructure,phase composition,hardness,density,wear resistance,bending strength and the fracture surface of multiphase metal-ceramics were studied by FE-SEM,EDS and XRD.The results show that,with the addition of a proper VC content,the grain growth of WCoB-TiC-Co multiphase metal-ceramics was effectively suppressed,and the toughness,fracture unevenness,bending strength,hardness and wear resistance of the materials were enhanced.When 0.9wt.% VC was added,the average grain size of WCoB-TiC-Co multiphase metal-ceramics was only 1.3 μm,and,the hardness and the bending strength were 91.5 HRA and 794 MPa,respectively.As the content of VC increased from 1.2wt.% to 1.5wt.%,the hardness,density,wear resistance and bending strength of WCoB-TiC-Co multiphase metalceramics reduced gradually.
参考文献
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%