通过分析南钢炼焦煤的煤岩性质和40 kg试验焦炉所炼焦炭抗碎强度,确定了基于炼焦煤镜质组最大反射率的活性权函数方程,根据其活性权函数对各炼焦煤的活惰比进行了计算,得出焦炭抗碎强度M40最大时所对应的活惰比为2.53,即为南钢用煤的最佳活惰比。以最佳活惰比为目标,优化配煤,预测焦炭质量,从而为科学便捷地确定配煤比提供技术依据。同时对非炼焦煤进行改性,使非炼焦煤具有一定的活性,非炼焦煤在炼焦中的配加量达到10%以上,炼制合格的焦炭。
Through the analysis of the coal and rock properties of coking coal,and testing the coke crushing strength in the 40 kg coke oven,the study identified the reactive weight function based on the coking coal vitrinite maximum reflec-tivity. The reactive-inert component radio of coking coal base on the active weight function was calculated,and it is con-cluded that the reactive-inert component radio correspond to the maximum crushing strength of coke. As the result of ex-periment analysis and calculation,the value of best reactive-inert component radio is 2.53. Aiming to reach the best reac-tive-inert component radio,the study optimized the ratio of mixing coal,predicted the coke quality,and provided techni-cal basis to determine coal blending ratio conveniently. At the same time,modification of non-coking coal makes the non-coking coal contain certain activity,and the optimal proposal of coal blending of non-coking coal can add up to 10%at least,be helpful to get qualified coke.
参考文献
[1] | 廖占平,朱子宗.我国非炼焦煤在炼焦中的应用[J].燃料与化工,2009(06):9-12. |
[2] | 任玉明.中国无烟煤资源与性质[J].洁净煤技术,2004(03):8-10. |
[3] | 范荣香.我国炼焦煤资源与煤焦化产业发展分析[J].化学工业,2008(05):1-8. |
[4] | 何选明.煤化学[M].北京:冶金工业出版社,2010.,2010. |
[5] | 张代林,余亮,郑明东.炼焦煤的煤岩特征对其结焦性质的影响[J].钢铁,2009(01):15-18,30. |
[6] | 钱晖,周渝生.煤与废塑料共焦化试验研究[J].钢铁,2010(01):96-98,103. |
[7] | 项茹,薛改凤,詹立志,陈鹏,鲍俊芳.增加弱黏结性炼焦煤配用比例的控制技术[J].钢铁,2013(09):21-25,44. |
[8] | 姚昭长.炼焦学[M].北京:冶金工业出版社,1995.,1995. |
[9] | 肖文钊,叶道敏.煤岩学配煤及其应用[J].煤质技术,2002(03):44-46. |
[10] | 戴中蜀.煤显微组分活性加权法预测焦炭质量和配煤粘结性[J].燃料与化工,1989(1):59.,1989. |
[11] | 朱子宗.一种复合煤粉改性剂、使用该复合煤粉改性剂制备的改性煤及该改性煤的制备方法:中国,ZL201310082891.5[P]. 2013-03-30.,2013. |
[12] | 廖占平,朱子宗,刁岳川,盛建文,王鑫海,杨舫.煤粉改性剂对非炼焦煤配煤炼焦的影响[J].钢铁,2010(07):13-16. |
[13] | 陈洪博,白向飞,王大力,姜英.焦炭光学组织与煤、焦质量关系研究[J].洁净煤技术,2009(06):78-81. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%