利用常用的轧制设备,采用热轧与冷轧及热处理相结合,提出了深度轧制工业纯铁和制备块体纳米晶工业纯铁的方法经X射线衍射(XRD)分析,深度轧制后的样品在300℃回复7 h,表层晶粒尺寸为38.9 nm;透射电镜(TEM)分析表明,板材内部的晶粒尺寸为87.5 nm.采用该方法可制备出大块、无孔隙缺陷的纳米晶工业纯铁,且晶粒的热稳定性较好.

参考文献

[1] Gleiter H. Prog Mater Sci, 1989; 33:223
[2] Koch C C. Nanostruct Mater, 1993; 2:109
[3] Birringer R, Gleiter H, Klein H P, Marquardt P. Phys Lett,1984; 102A: 356
[4] Lu K. Mater Sci Eng, 1996; 16R: 161
[5] Erb U, El-Sherik A M, Palumbo G, Aust K T. Nanostruct Mater, 1993; 2:383
[6] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45:103
[7] Lu K, Lu J. J Mater Sci Technol, 1999; 15:193
[8] Jain M, Christman T. J Mater Res, 1996; 11:2677
[9] Song P C, Wei G. The Production Technology of Plate Steel. Xi'an: Xi'an Jiaotong University Press, 1989:159(宋佩莼,韦光.板带钢生产工艺学.西安:西安交通大学出版社,1989:159)
[10] Zhao Y Z. Plastic Deformation and Rolling Theory of Metals. Beijing: Metallurgical Industry Press, 1980:72(赵业志.金属塑性变形与轧制理论.北京:冶金工业出版社,1980: 72)
[11] Li M Y, Sun B R. The Technique Handbook of Control Rolling and Control Cooling for Steel. Beijing: Metallurgical Industry Press, 1998:3(李曼云,孙本荣.钢的控制轧制和控制冷却技术手册北京:冶金工业出版社,1998:3)