利用电磁离心铸造(EMCC)工艺制备NiAl/Cr(Mo)共晶合金,研究了合金的显微组织和压缩性能.结果表明,合金显微组织细小,由激冷区、共晶区和亚共晶区组成.激冷区以初生β-NiAl相为主,共晶区由β-NiAl和α-Cr(M0)相构成,亚共晶区由初生β-NiAl和β-NiAl/Q-Cr(Mo)共晶组成.EMCC NiAl共晶合金1000℃压缩行为遵从幂指数规律:ε=Aσn.合金的室温断裂方式以基体NiAl的解理断裂和NiAl/Cr(Mo)的相界面剥离为主.
参考文献
[1] | Johnson D R, Chen X F, Oliver B F, Noebe R D, Whittenberger J D. Intermetallics, 1995; 3:99 |
[2] | Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10:1159 |
[3] | Darolia R. Intermetallics, 2000; 8:1321 |
[4] | Raj S V, Locci I E, Whittenberger J D. In: Hemker K J,Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M,Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics 2001, TMS, 2001:785 |
[5] | Whittenberger J D, Locci I E, Raj S V, Salem J A. Metall Mater Trans, 2002; 33A: 1385 |
[6] | Cui C Y, Guo J T, Qi Y H, Ye H Q. Mater Trans, 2001;42:1700 |
[7] | Cui C Y, Guo J T, Qi Y H, Ye H Q. Intermetallics, 2002;10:1001 |
[8] | He Y L, Yang Y S, Hu Z Q. Mater Rev, 2000; 14(7): 3(贺幼良,杨院生,胡壮麒.材料导报,2000;14(7):3) |
[9] | Qiu Y Q, Wang X, Jia G L, Gao Y Y, Yang H C. J Northeasten Univ (Natural Sci), 2000; 21:181(邱以清,王溪,贾光霖,高允彦,杨洪才.东北大学学报(自然科学版),2000;21:181) |
[10] | Guo D Y, Yang Y S, Tong W H, Hua F A, Cheng G F,Hu Z Q. Acta Metall Sin, 2003; 39:914(郭大勇,杨院生,童文辉,花福安,程根发,胡壮麒.金属学报.2003;39:914) |
[11] | Lin G, Yang Y S, Hua F A, Guo D Y, Hu Z Q, Acta Metall Sin, 2003; 39:1233(林刚,杨院生,花福安,郭大勇,胡壮麒.金属学报.2003;39:1233) |
[12] | Chen Y X, Cui C Y, He L L, Guo J T, Li D X. Acta Metall Sin, 1999; 35:897(陈玉喜,崔传勇,贺连龙,郭建亭,李斗星.金属学报,1999;35:897) |
[13] | Walston W S, Darolia R. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D, eds., Structural Intermetallics 2001, TMS, 2001:735 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%