能保持较高的Al含量,使得涂层能抵抗更长时间的高温氧化.
参考文献
[1] | Jeanine T D,Dinesh K G.Surf Coat Technol,1994; 68-69:1 |
[2] | Goward G W.Surf Coat Teehnol,1998; 108-109:73 |
[3] | Nicholls J R.Mater Res Bull,2003; 28:1 |
[4] | Brandl W,Grabke H J,Toma D,Kruger J.Surf Coat Technol,1996; 86-87:41 |
[5] | Wu Y N,Qin M,Feng Z C,Liang Y,Sun C,Wang F H.Mater Left,2003; 57:2404 |
[6] | Tang F,Ajdelsztajn L,Sehoenung J M.Oxid Met,2004;61:219 |
[7] | Wang B,Gong J,Sun C,Huang R F,Wen L S.Mater Sci Eng,2003; A357:39 |
[8] | Guo M H,Wang Q M,Ke P L,Gong J,Sun C,Huang R F,Wen L S.Surf Coat Technol,2006; 200:3942 |
[9] | Smeggil J G.Mater Sci Eng,1987; A87:261 |
[10] | Sun C,Wang Q M,Tang Y J,Guan Q F,Gong J,Wen L S.Acta Metall gin,2005; 41:1167(孙超,王启民,唐永吉,关庆丰,宫骏,闻立时.金属学报,2005;41:1167) |
[11] | Tolpygo V K,Clarke D R.Acta Mater,1999; 47:3589 |
[12] | Dryepondt S,Clarke D R.Scr Mater,2009; 60:917 |
[13] | Prescott R,Graham M J.Oxid Met,1992; 38:233 |
[14] | Li M S.High Temperature Corrosion of Metals.Beijing:Metallurgical Industry Press,2001:37(李美栓.金属的高温腐蚀.北京:冶金工艺出版社,2001:37) |
[15] | Itoh Y,Saitoh M,Ishiwata Y.J Mater Sei,1999; 34:3957 |
[16] | Knotek O,LSfiter F,Beele W.Surf Coat Technol,1993;61:6 |
[17] | Lou H Y,Wang F H.Vacuum,1992; 43:757 |
[18] | Wang Q M,Zhang K,Gong J,Cui Y Y,Sun C,Wen L S.Acta Mater,2007; 55:1427 |
[19] | Maxim K,David H P,Christoph T,Hans-Peter B,Christoph S.US Pat,US6 383 312,2002 |
[20] | Sakata M,Hayashi S,Nishimoto T,Yoshioka T,Narita T.Oxid Met,2007; 68:295 |
[21] | Sumoyama D,Thosin K Z,Nishimoto T,Yoshioka T,Izumi T,Hayashi S,Narita T.Oxid Met,2007; 68:313 |