采用醋酸锰和醋酸锂作为起始反应物,在水溶液中混合均匀,通过加热蒸发形成混合均一的反应前趋体并在不同温度下焙烧可获得最终产物.在850°C下,起始反应物锂锰摩尔比例采用1.1:2可获得电化学性能较好的活性材料.利用热重分析及红外光谱对反应历程进行分析并提出了可能的反应机理.对所合成的产物进行XRD、结构形貌及电化学性能进行测试研究,表明其颗粒细小、分布均匀、结晶性能好、为蜂窝状结构、比表面积较大,初始容量较高和循环稳定性能良好,初始容量达128mAh/g.
参考文献
[1] | NagauraT, Ozawa K T. Prog. Batt. Scol. Cells, 1990, 9: 209. |
[2] | Hunter James C. J. Solid State Chem. 1981, 39: 142-147. |
[3] | Tarascon J M, Wang E, Shokoohi F K, et al. J. Electrochem. Soc. 1991, 138: 2859-2864. |
[4] | Tarascon J M, Mckinnon W R, Coowar F, et al. ibid. 1994, 141: 1421-1431. |
[5] | Yoshio M, Inoue S, Hykutake M, et al. J. Power Sources, 1991, 34: 147-152. |
[6] | Yoshio M, Noguchi H, Miyashita T, et al. J. Power Sources, 1995, 54: 483-486. |
[7] | Huang Haitao, Bruce Peter G. J. Electrochem. Soc. 1994, 141 (9): L106-L109. |
[8] | Liu W, Kowal K, Farrington G C. ibid. 1996, 143: 3590-3596. |
[9] | Herna Lourdes, Morales Julian, Sanchez Luis, et al. Solid State Ionics, 1999, 118: 179-185. |
[10] | Hernan L, Morales J, Sanchez L, et al. ibid. 1997, 104: 205. |
[11] | Sun Yang-Kook. ibid. 1997, 100: 115-125. |
[12] | Barboux P, Manthirm J M, Schokoohi F K. J. Solid State Chem. 1991, 94: 185-196. |
[13] | Reimers J N, Eric W Fuller, Dahn J R. J. Electochem. Soc. 1993, 140: 3396-3401. |
[14] | Kim J, ManthiamA. Nature, 1997, 390 (20): 265-267. |
[15] | Naghash A R, Lee Jim Y. J. Power Sources. 2000, 85: 284-293. |
[16] | Pasquier A Du, Blyr A, Courjal P, et al. J. Electochem. Soc. 1999, 146: 428-436. |
[17] | Tarascon J M, Mckinnon W R, et al. J. Electrochem. Soc. 1994, 141: 1421-1431. |
[18] | Yamada A, Miura K, et al. ibid. 1995, 142: 2149-2156. |
[19] | SunYang-Kook, Lee Kyeong-Hee, et al, Solid State Ionics, 1998, 112: 237-243. |
[20] | Yang Wensheng, Liu Qingguo, et al. ibid. 1999, 121: 79-84. |
[21] | 杨文胜,刘庆国,等.电源技术(Chinese Journal of Power Sources),1999,23:49-52 |
[22] | Peramunage D, Abraham K M. J. Electrochem. Soc. 1998, 145: 1131-1136. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%