层状复合陶瓷材料是目前陶瓷增韧的最有效途径之一,有着广泛的应用前景,是陶瓷增韧研究的热点,近年来发展很快.本文介绍了层状复合陶瓷材料的结构设计、制备、特点以及主要韧化机制,综述了几种不同体系层状复合陶瓷材料的国内外研究进展情况,并探讨了层状复合陶瓷材料的弱点及今后应进一步研究的若干问题.
参考文献
[1] | Wang R Z, Wen H B. J. Mater. Sci., 1995, 30: 2299. |
[2] | Huang L J, Li H D. Mater. Res. Soc. Symp. Proc., 990, 174: 101. |
[3] | Chartier T, Merle D. J. Eur. Ceram. Soc., 1995, 15 (2): 101-107. |
[4] | Wojciech S, Masatomo Y. Key Eng. Mater., 1997, 132-136(Pt 3): 2025-2028. |
[5] | Calcvert P. Mater. Res. Soc. Symp. Proc., 1990, 180: 619. |
[6] | Kovar D, Michael T. J. Am. Ceram. Soc., 1997, 80 (3): 673-679. |
[7] | 蔡胜有,李金林,谢志鹏,等.复合材料学报,1999,16(2):110-115. |
[8] | 张志强,尚成嘉,职任涛.材料研究学报,1995,9(5):477-479. |
[9] | Kaya C, Kaya F, Boccaccini P A, et al. Ceram. Intermational, 1999, 25: 359-366. |
[10] | Yue X M, Zhang G J, Watanabe T. J. Eur. Ceram. Soc., 1999, 19 (3): 293-298. |
[11] | Russo C J, Harmer M P, Chan H M, et al. J. Am. Ceram. Soc., 1992, 75 (12): 3396-3400. |
[12] | Ham S R, Wilkinson D S. J. Am. Ceram. Soc., 1995, 78 (6): 1580-1584. |
[13] | Liu H, Hsu S M. J. Am. Ceram. Soc., 1996, 79 (9): 2452-2457. |
[14] | Shigegaki Y. J. Am. Ceram. Soc., 1997, 80 (10): 2624-2628. |
[15] | Ohji T, Shigegaki Y, Kondo N, et al. Mater. Lett., 1999, 40: 280-284. |
[16] | Ohji T, Shigegaki Y, Miyajima T, et al. J. Am. Ceram. Soc., 1997, 80 (4): 991-994. |
[17] | Oechsner M, Hillman C, Lange F. J. Am. Ceram. Soc., 1996, 9 (7): 1834-1838. |
[18] | Shigegaki Y. J. Am. Ceram. Soc., 1996, 79 (8): 2197-2200. |
[19] | Manuel J M, Carolina C. J. Am. Ceram. Soc., 1997, 80 (8): 2126-2130. |
[20] | Requena J, Moreno R, Moya J S. J. Am. Ceram. Soc., 1989, 72 (8): 1511-1513. |
[21] | Sanchez A J, Moya J S, Tomsia A P. J. Mater. RES, 1996, 8 (2): 113-114. |
[22] | Harmer M P, Chan H M, Miller G A. J. Am. Ceram. Soc., 1992, 75 (7): 1715-1720. |
[23] | 钱晓倩,葛曼珍,吴义兵,等(QIAN Xiao-Qian,et al).无机材料学报(Journal ofInorganic Materials),1999, 14 (4): 520-526. |
[24] | Clegg W J. Acta Metall. Mater., 1992, 40 (11): 3085-3093. |
[25] | 罗永明,潘伟,陈健,等.材料导报,2000,14(5):49-51. |
[26] | Zhang C, Mecholsky J J. J. Mater. RES, 1993, 8 (9): 20-25. |
[27] | Sarakiya M. MRS Symp. Proc., 1990, 174: 109-124. |
[28] | He J L, Li W Z, Liu C H. Surf. Coat. Technol., 1998, 103 (5): 276-280. |
[29] | Wang R L. Chinese Journal of Mat. Res., 1996, 10 (1): 95-100. |
[30] | Tomaszewski H. J. Eur. Ceram. Soc., 1999, (19): 1329-1331. |
[31] | Cook J, Gordon J E. Proc. R. Soc., 1964, A282: 508. |
[32] | Favre J P. J. Mater. Sci., 1977, 12: 43-48. |
[33] | Clegg W J. Nature, 1990, 347 (4): 455-461. |
[34] | Zhang L, Krstic V D. Theoret. Appl. Fract. Mech., 1995, 24: 13-20. |
[35] | Padture N P, Pender D C, Wuttiphan S, et al. J. Am. Ceram. Soc., 1995, 78 (11): 3160-3162. |
[36] | Kovar D, Thouless M D, Halloran J W. J. Am. Ceram. Soc., 1998, 81 (4): 1004-1011. |
[37] | Huang Y, Hao H N, Chen Y L, et al. Acta Metall. Sinica, 1996, 9 (6): 479-484. |
[38] | Wang C, Huang Y, Zan Q F. Mater. Sci. Eng., 2000, 11: 9-12. |
[39] | She J, lnoue T, Ueno K. Ceram. International, 2000, 26: 801-805. |
[40] | She J, lnoue T, Ueno K. J. Eur. Ceram. Soc., 2000, 20 (11): 1771-1775. |
[41] | Katsoki H. Ceram. Soc. Jap., 1993, 101 (9): 1068-1071. |
[42] | Boch P, Chartier C. J. Am. Ceram. Soc., 1996, 79 (8): 1734-1738. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%