为了扩大锂离子电池正极材料LixMn2O4的工作电压范围,在保证良好循环性能的基础上提高材料的容量,本文对S-Co复合掺杂LiMn2O4的合成工艺和电化学性能进行了研究.溶胶-凝胶法合成的各试样均为纯的立方尖晶石相,且结晶状态良好.S-Co复合掺杂综合了S掺杂效应和Co掺杂效应,改善了LiMn2O4的电化学性能,在2.4~4.3V充放电压范围内,初始容量较高,达到170 mAh/g,30次循环后容量不但没有衰减而且有一定增加.

参考文献

[1] Tsutomu Ohzuku, Sachio Takeda, et al. J. Power sources, 1999, 81-82: 90-95.
[2] West K, Vitins G, et al. Electrochimica Acta, 2000, 45: 3141-3147.
[3] 夏君磊,等.S掺杂LiMn2O4尖晶石的合成与性能,电池.
[4] Sang Ho Park, Ki Soo Park, et al. J. Electrochem. Soc., 2000, 147: 2116-2121.
[5] Sun Yang-Koo. Electrochemistry Communication, 2001, 3: 199-202.
[6] Sun Yang-Koo, Gyeong-Su Park, et al. J. Electrochem. Soc., 2001, 148: A994-A998.
[7] Sun Yang-Koo, Bookeun Oh, et al. Electrochimica Acta, 2000, 46: 541-546.
[8] Amarilla J M, Martin J L, et al. Solid State Ionics, 2000, 127: 73-77.
[9] Kanamura S, Toriyama S, Shiraishi Z I. J. Electrochem. Soc., 1995, 142 (i): 1383-1389.
[10] Amatucci G G, Pereira N, et al. J Power Sources, 1999, 39-43: 39-43.
[11] Lubomir B, Jean-Luc B, et al. J. Solid State Chemistry, 1999, 145: 503-510.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%