以活性炭为载体,采用溶胶-凝胶法制备了TiO2/活性炭(TiO2/AC)复合体,并利用SEM和XRD手段对复合体进行表征,通过Dt2=ktnexp(-E/RT)方程的计算,分析,研究活性炭对复合体中TiO2晶粒生长及其相变的影响.结果表明:TiO2/AC复合体晶粒粒径增长的时间比TiO2本体短;TiO2/AC复合体纳米粒子平均尺寸为50nm比TiO2本体小;锐钛矿向金红石转变的相变温度和晶粒生长最快温度TiO2/AC复合体比TiO2本体高.锐钛矿和金红石晶粒生长的表观活化能TiO2/AC复合体分别为6.21±1.27和46.54±1.56kJ/mol,TiO2本体分别为5.764±1.02和36.4±1.14kJ/mol.在锐钛矿阶段和金红石阶段TiO2/AC复合体反应指数分别为0.19和0.35,而TiO2本体分别为0.13和0.26.原因是活性炭的强吸附力和非晶相层对TiO2晶粒生长的阻遏作用.
参考文献
[1] | Kawasaki K, Despres J F, Kamei S, et al. J. Mater. Chem., 2002, 16: 2117-2124. |
[2] | 张青红,郭景坤(ZHANG Qing-Hong,et al).无机材料学报(Journal of Inorganic Materials),2000,15(3):556-560. |
[3] | 吴风清,阮圣平,李小平(WU Feng-Qing,et al).高等学校化学学报(Chemical Journal of Chinese Unversities),2000,21:1578-1580. |
[4] | Zhang Q H, Gao L, Guo J K. Appl. Catal. B: Environ., 2000, 26: 207-218. |
[5] | Paz Y, Heller A. J. Mater. Res., 1997, 12: 2759-2766. |
[6] | Kato K, Tsuzuki A, Torii Y, et al. J. Mater. Sci., 2000, 36: 890-897. |
[7] | 苏碧桃,常玥,张力(SU Bi-Tao,et al).高等学校化学学报(Chemical Journal of Chinese Unversities),2003,24:892-894. |
[8] | Byrne J A, Eggins B R, Brow N M D, et al. J. Appl. Catal. B: Environ., 1998, 17: 83-92. |
[9] | Wang R, Hashimoto K, Fujishima A, et al. Adv. Mater., 1998, 10: 135-138. |
[10] | Tokeda N, Tcrimoto T, Sampath S, et al. J. Phys. Chem., 1995, 99: 9986-9991. |
[11] | Sampath S, Uchida H,Yoneyama H. J. Catal., 1994, 149: 189-194. |
[12] | Torimoto T, Ito S, Kuwabata S, et al. Enrivon. Sci. Technol., 1996, 30: 1275-1281. |
[13] | 廖振华,陈建军(LIAO Zhen-Hua,et al).无机材料学报(Journal of Inorganic Materials),2004,19(1):17-24. |
[14] | Hoffmann M R, Martin S, Choi W, et al. J. Chem. Rev., 1995, 95 (1): 69-96. |
[15] | Trapali C, Kozhukharov V, Samuneva B, et al. J. Mater. Sci., 2000, 36: 1275-1283. |
[16] | Ohtani B, Iwai K, Nishimoto S, et al. J. Phys. Chem. B., 1997, 101: 3349-3359. |
[17] | Spurr R A, Myers H. J. Anal. Chem., 1957, 29: 760-762. |
[18] | Eastman J A. J. Appl. Phys., 1994, 75: 770-779. |