通过SEM、TEM及硬度和拉伸性能测试对SiCW/6061Al复合材料正挤压管材和反挤压杯的组织和性能进行了观察和测定.研究结果表明,挤压使SiCW发生了定向排列和折断,挤压温度是影响挤压件组织和性能的重要因素,挤压件硬度分布不均匀是由于金属流动不均匀所致,挤压后固溶时效处理能够大幅度地提高复合材料的抗拉强度.

参考文献

[1] Mohn W R, Vukotratovich D. Recent applications of metal matrix composites in precision instruments and optical systems. J Materials Engineering, 1988,10(3):225
[2] Mohn W R, Vukotratovich D. Engineered metal matrix composites for precision optical systems. SAMPE J, 1988(1~2):26
[3] 耿林. 压铸SiCW/LD2复合材料中晶须及界面的微观结构: [博士学位论文]. 哈尔滨工业大学,1990
[4] 刘宗荣. SiCW/Al复合材料界面区结构和形变断裂过程: [博士学位论文]. 哈尔滨工业大学,1994
[5] Liu Y L. A study on flow stress of Al-SiC composites deformed in large range of strain. Script Materialia, 1996, 35(2): 253~259
[6] Stanford-Beale C A, Clyne T W. Extrusion and high-temperature deformation of fibre-reinforced aluminium. Composites Science and Technology, 1989, 35: 121~157
[7] Suganuma K, Fujita T, Niihara K. Hot extrusion of AA7178 with AL2O3 fibre. Materials Science and Technology, 1989, 5(3):249~254
[8] 汪大年. 金属塑性成形原理. 北京: 机械工业出版社, 1982.161~162
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%