采用高功率脉冲磁控放电等离子体注入与沉积(HPPMS-PIID)和常规直流磁控溅射复合的方法设计制备了包含高结晶度的CrN纳米粒子的DLC薄膜,并对不同C靶电流时制备的CrN-DLC薄膜的形貌、结构及性能进行了研究.结果表明,随C靶电流的增加,薄膜中的含C量增加,在较高的C含量时形成了明显的DLC薄膜特征,掺杂相主要成分为高度200择优取向的CrN纳米晶,其最小晶粒尺寸为42.39 mn.薄膜中的C主要以C-sp2,C-sp3和CN-sp3键的形式存在,sp3键的总含量为sp2总含量的44.8%.所制备的薄膜具有很好的膜基结合力(临界载荷Lc=66.8 N)和较高的纳米硬度(最高达24.3 GPa).
参考文献
[1] | Liang F,Yan X.J.Acta Phys Sin,1999; 48:1095(梁风,严学俭物理学报,1999; 48:1095) |
[2] | Grill A.Diamond Relat Matcr,1999; 8:428 |
[3] | Chcn G H,Yan S G,Zhang F Q.Acta Phys Sin,1992; 41:500(陈光华,阎少光,张仿清.物理学报,1992;41:500) |
[4] | Schwarz C,Heeg J,Rosenberg M,Wienecke M.Diamond Relat Mater,2008; 17:1685 |
[5] | Takeno T,Hoshi Y,Miki H,Takagi T.Diamond Relat Mater,2008; 17:1669 |
[6] | Gu K M,Tang J N,Li J Q,Yang Q P.J Shenzhen Univ Sci Eng,2007; 24:159(谷坤明,汤皎宁,李均钦,杨钦鹏.深圳大学学报理工版,2007;24:159) |
[7] | Nie C Y,Zhang B Y,Xie H M.Acta Metall Sin,2007; 43:1207(聂朝胤,张碧云,谢红梅.金属学报.2007; 43:1207) |
[8] | Veprek S,Argon A S.Surf Coat Technol,2001:146 147:175 |
[9] | Mourae Silva C W,Branco J R T,Cavaleiro A.Thin Solid Films,2006; 515:1063 |
[10] | Baba K,Hatada R,Tanaka Y.Surf Coat Technol,2007;19-20:8362 |
[11] | Tian X B,Wu Z Z,Gong C Z,Yang S Q.Chin Pat,201010213894.4,2010(田修波,吴忠振,巩春志,杨士勤.中国专利,201010213894.4,2010) |
[12] | Kouznetsov V,Macádk K,Schneider J M,Helmersson U,Petrov I.Surf Coat Technol,1999; 122:290 |
[13] | Helmersson U,Lattemann M,Bohlmark J,Ehiasarian A P,Gudmundsson J T.Thin Solid Films,2006; 513:1 |
[14] | Wu Z Z,Tian X B,Shi J W,Yang S Q,Chu P K.Rev Sci Irst,2011; 82:033511 |
[15] | Wu Z Z,Tian X B,Wang Z M,Gong C Z,Yang S Q.Chin J Vac Sci Technol,2011; 31:1(吴忠振,田修波,王泽明,巩春志,杨士勤.真空科学与技术学报,2011; 31:1) |
[16] | Li G,Xia L F,Ma X X,Sun Y,Zhan Z J.Acta Metall Sin (Eng Lett),1999; 12:551 |
[17] | Ji H B,Xia L F,Ma X X,Sun Y,Sun M R.Acta Metall Sin (Eng Lett),2000; 13:967 |
[18] | Wu Z Z.Master Dissertation,Harbin Institute of technology,2008(吴忠振,哈尔滨工业大学硕士学位论文,2008) |
[19] | Tian X B,Wu Z Z,Shi J W,Li X P,Gong C Z,Yang S Q.Vacuum,2010; 47:44 田修波,吴忠振,石经伟,李希平,巩春志,杨士勤.真空,2010;47:44) |
[20] | Anders A.Surf Coat Technol,1997; 93:158 |
[21] | Martin P J,Bendavid A,Cairney J M,Hoffman M.Surf Coat Technol,2005; 200:2228 |
[22] | Ma D Y,Ma S L,Xu K W.Acta Metall Sin,2004; 40:1037(马大衍,马胜利,徐可为.金属学报,2004; 40:1037) |
[23] | Guo Y,Xu B,Wu G Z,Ma S L,Xu K W.Acta Metall Sin,2007; 43:159(郭岩,徐彬,吴贵智,马胜利,徐可为,金属学报,2007:43:159) |
[24] | Alami J,Sarakinos K,Uslu F,Wuttig M.J Phys D:Appl Phys,2009; 42:015304 |
[25] | Vyas A,Shen Y G,Zhou Z F,Li K Y.Compos Sci Technol,2008; 68:2922 |
[26] | Shi Y,Long S,Liang F.Appl Surf Sci,2008; 254:5861 |
[27] | Yang Y Y,Peng Z J,Fu Z Q,Wu S D,Chen X C,Wang C B.Acta Metall Sin,2010; 46:34(杨义勇,彭志坚,付志强,邬苏东,陈新春,王成彪.金属学报.2010; 46:34) |
[28] | Yang W J,Choa Y-H,Sekino T,Shim K B,Niihara K,Auh K H.Thin Solid Films,2003; 434:49 |
[29] | Jiang B L,Hu P F,Li H T.Trans Mater Heat Treat,2010;31:134(蒋百灵,胡鹏飞,李洪涛.材料热处理学报.2010; 31:134) |
[30] | Niu S C,Yu Z M,Dai M J,Lin S S,Hou H J,Li H W.China Surf Eng,2007; 20:34(牛仕超,余志明,代明江,林松盛,候惠君,李洪武.中国表面工程.2007; 20:34) |
[31] | Veprek S,Niederhofer A,Moto K,Bolom T,Mannling H-D,Nesladek P,Dollinger G,Bergmaier A.Surf Coat Technol,2000; 133-134; 152 |
[32] | Robertson J.Mater Sci Eng,2002; R37:129 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%