以无压烧结工艺制备了Si3N4/SiO2复合材料. 实验结果表明: Si3N4颗粒对石英基体的析晶起到了抑制作用和增韧补强作用. Si3N4含量为5vol%的样品在1370℃烧结2h后, 抗弯强度达到96.2MPa, 断裂韧性为2.4MPa·m1/2, 介电常数和介电损耗分别在3.63~3.68和1.29~1.75×10-3之间.

Si3N4/SiO2 composites were prepared with pressureless sintering. It was found that the Si3N4 particle was effective to suppress the crystallization of cristobalite in the Si3N4/SiO2 composites and contributed to the improvement of the mechanical properties. After sintered at 1370℃ for 2h, the flexural strength of the composites with 5vol% Si3N4 addition reached 96.2MPa, the fracture toughness was 2.4MPa·m1/2. The dielectric constant and loss tangent of the composites was 3.63~3.68 and 1.29~1.75×10-3, respectively.