以2,4,6,8-四甲基环四硅氧烷和乙烯基三甲氧基硅烷为原料,通过硅氢与乙烯基的加成反应一步合成了新型环状结构前驱体.前驱体与正硅酸乙酯(TEOS)在酸性条件下发生水解-缩合反应,制得了一种具有环状体型结构的新型有机-无机杂化涂料.采用FT-IR对合成的前驱体及杂化涂料进行了结构表征.热失质量(TG)分析表明,杂化涂料的热稳定性良好.随TEOS用量的增加,杂化涂料的热稳定性提高.杂化涂料对金属的附着力1级,光泽>130,铅笔硬度5 H~6 H,耐冲击性>50 cm.250g/200r耐磨性试验磨损值为0.003 g,显示出优异的耐磨性能.

参考文献

[1] JentschJD;Mager M;Mechtel M et al.Multi - functional, Cyclic Organosiloxanes, Process for The Production Thereof and Use Thereof[P].US:6005131,1999-12-21.
[2] KrausH;Leverkusen;Mechtel M et al.Process for Preparation of Sioh - functional Carbosilane Dendrimers[P].US:5880305,1999-03-09.
[3] MagerM;Leverkusen;Hofacker S et al.Boron - and/or Aluminum - containing Mixtures, Hybrid Materials, and Coatings[P].US:6395826,2002-05-28.
[4] Karl-Heinz Haas;Sabine Amberg-Schwab;Klaus Rose .Functionalized coating materials based on inorganic-organic polymers[J].Thin Solid Films: An International Journal on the Science and Technology of Thin and Thick Films,1999(1/2):198-203.
[5] Voevodin N.;Simon L.;Khobaib M.;Donley M.;Jeffcoate C. .Characterization of pitting corrosion in bare and sol-gel coated aluminum 2024-T3 alloy[J].Surface & Coatings Technology,2001(1):29-34.