用还原焙烧法从硫铁矿烧渣中提取铁,制得FeSO4,并以其为原料,在初始铁离子浓度c(Fe2+)为0.15~0.25mol/L、n(Na2CO3)/n(FeSO4)=1的近中性条件(pH值为6~7)下,制备了α-FeOOH晶核;滴加Na2CO3溶液以中和生成α-FeOOH时释放的H+,控制溶液pH值为4~5,使Fe2+以适宜的氧化速率在α-FeOOH晶核的外延生长,制得了均匀性较好的针状α-FeOOH晶体(宽30~40 nm、长约为250 nm).

参考文献

[1] ZHENG Ya-Jie(郑雅杰),GONG Zhu-Qing(龚竹青),CHEN Bai-Zhen(陈白珍),et al.Tech Equip Environ Pollun Cont(环境污染治理技术与设备)[J],2001,2(1):48
[2] Wohlfarth E P. Ferromagnetic Materials Vol. 2[ M]. New York:Noeth-Holland Publishing Company,1980:406
[3] Craik D J. Magnetic Oxides Part 2 [ M ]. London: John Wiley & Sons, 1975:697
[4] Sada E,Kumazawa H,Aoyama M. Chem Eng Comm[J],1988,71:73
[5] Harada S J, Fujimoto S R, Okuda K O. Koukai Tokyo Kouhou( A), Hei 2-172826,1990
[6] Harada S J,Fujimoto S R,Okuda K O. Koukai Tokyo Kouhou(A) ,Hei 2-172827,1990
[7] ZENG Heng-Xing(曾恒兴),ZHANG Shu-Yuan(张庶元),LIU Guang-Song(刘光松),et al.Chin Sci Bull(科学通报)[J],1994,39(4):319
[8] LIN Bi-Xia(林碧霞),ZHANG Shu-Yuan(张庶元),TAN Yu(潭舜),et al.Chin Ceramic Soc(硅酸盐学报)[J],1995,23(1):33
[9] CAI Sh-Yin(蔡世银),CHE A-Xiao(车阿小),LI Chun-Zhong(李春忠),et al.J East Chin Univ Sci Tech(华东理工大学学报)[J],1997,23(2):298
[10] Morales M P,Tartaj P,Serna C J. JMater Chem[J] ,2000,10(11) :2 561
[11] Yutuka T. J Chem Soc Dolton Trans[J] ,1981,197:1 807
[12] Detournay J. Corrosion Sci[J] ,1975,15:295
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%