研究了冷轧IF钢板镀锌前后的热电势(TEP)特性。试 验结果表明:镀锌退火后,钢板基体发生再结晶导致TEP值升高,而镀层的形成导致TE P值下降,基体的再结晶起主导作用。并且,TEP值存在各向异性,这与钢板的织构有关 。
This paper deals with the thermoelectric power ( TEP) characteristics of an interstitial-free (IF) steel sheet before and after the galvanizng processing. Recrystallization of the matrix increases the TEP va lue, and formation of the coating decreases the TEP value. TEP values of the IF steel sheet reflect the anisotropy present in the sheet. These are related t o the changes in sheet texture.
参考文献
[1] | MasaruSagiyama;Jun-ichi Inagaki;Masaya Morita.Fe-Zn allo y ing behaviour and coating microstructrue of galvanized steel sheets (63)[J].NKK Te chnical Resiew,1991(63) |
[2] | InagakiJ;Morita M;Sagiyama M .Iron-zinc alloying react ion of interstitial-free steels[J].Surface Engineering,1991,7(04):331-339. |
[3] | NorthwoodDO;Robinson J W;Jie Z.The use of thermoelectric power measurements to study recovery,recrystallization and phase transformation s in cold-worked Zr-1%Nb and zircaloy-4 nuclear fuel sheathing[J].Journal of Materials Engineering and Performance,1992(01):143-148. |
[4] | NorthwoodDO;Sun X-C;Hochreiter J.Thermoelectric po wer (TEP) measurements as a materials characterization technique.13th . Int. Conf. on Thermoelectricity,Ed. Mathiprakasam B[C].Kansas City:MidWe st Res.Inst.MO.B4-2,1994 |
[5] | BarnardRD.Thermoelectricity in Metals and Alloys[M].Lon don:Taylor and Francis,1972 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%