总结了工业中抗微动损伤的基本途径,指出了表面工程技术减缓微动损伤的重要作用,并从表面机械强化、扩散处理、表面化学处理、电沉积、热喷涂、气相沉积、高能密度处理和固体润滑涂层等表面工程分支综述了目前的研究现状.介绍了作者在径向和复合微动中的最新研究进展.
参考文献
[1] | Vincent L .Mechanics and materials in fretting[J].Wear,1992,153:135-148. |
[2] | Zhou Z R;Fayeulle S;Vincent L .Cracking behavior of various aluminium alloys during fretting wear[J].Wear,1992,155:317-330. |
[3] | Beard J.Palliative for fretting fatigue[A].London:Mechanical Engineering Publications,1994:419-436. |
[4] | Petiot C;Foulquier J;Journet B.Fretting fatigue behaviour of a chromium vanadium molybdenum steelinfluence of surface protection[A].London:Mechanical Engineering Publications,1994:497-512. |
[5] | Chakravarty S;Dyer J P;Conway Jr J C.Influence of surface treatments on fretting fatigue of Ti-6242 at elevated temperatures[A].West Conshohocken PA:American Society for Testing and Materials,2000:491-505. |
[6] | Gordelier S C;Chivers T C .A literature review of palliatives for fretting fatigue[J].Wear,1979,56:177-190. |
[7] | Waterhouse R B;Brook P A;Lee G M C .The effect of electrodeposited metals on the fatigue behaviour of mild steel under conditions of fretting corrosion[J].WEAR,1962,5:235-244. |
[8] | Murata H;Imada Y;Honda F et al.Effect of fretting on electroplated Pd-Ni contacts[J].Wear,1993,162-164:339-346. |
[9] | Rudolphi A K;Jacobson S .Gross plastic fretting-examination of the gross weld regime[J].Wear,1996,201:255-264. |
[10] | A. Ramalho;L. M. Correia;J. D. Costa .Fretting fatigue of zinc coated low carbon steel EN H320 M[J].Tribology International,2000(11):761-768. |
[11] | Okado J.;McColl I.R.;Waterhouse R.B.;Hasegawa T.;Kasaya M.;Shima M. .Ni-P and Mo: An excellent fretting wear resistant combination[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,1999(2):749-757. |
[12] | Fu Y Q;Batchelor A W;Khor K A .Fretting wear behaviors of thermal sprayed hydroxyapatite coating under lubricated with bovine albumin[J].Wear,1999,230:98-102. |
[13] | Waterhouse R B.Plastic deformation in fretting processes-a review[A].West Conshohocken PA:American Society for Testing and Materials,2000:3-18. |
[14] | Wit E de;Blanpain B;Froyen L et al.Tribochemical behaviour of TiN-coatings during fretting wear[J].Wear,1998,217:215-224. |
[15] | Batchelor A W;Stachowiak G W;Stachowiak G B et al.Control of fretting friction and wear of roping wire by laser surface alloying and physical vapour deposition coatings[J].Wear,1992,152:127-150. |
[16] | Waterhouse R B;Iwabuchi A.The compositional properties of surface films formed during the high temperature fretting of titanium alloys[A].Tokyo,Japan,1985 |
[17] | Zhu MH.;Zhou ZR. .An investigation of molybdenum disulfide bonded solid lubricant coatings in fretting conditions[J].Surface & Coatings Technology,2001(2/3):240-245. |
[18] | 朱旻昊 .径向与复合微动的远行和损伤机理研究[D].西南交通大学,2001. |
[19] | Zhu MH.;Kapsa P.;Vincent L.;Zhou ZR. .Radial fretting fatigue damage of surface coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2001(1):650-657. |
[20] | M. H. Zhu;Z. R. Zhou;Ph. Kapsa;L. Vincent .An experimental investigation on composite fretting mode[J].Tribology International,2001(11):733-738. |