为了提高铝合金表面的耐蚀性和与有机涂层的粘接耐久性,首先对铝合金进行水煮(65℃、15 min)处理,在其表面形成富含羟基氢氧化物层,然后经两步浸涂后再高温固化(100℃×60min),在被氧化的铝合金表面形成了双-[3-(三乙氧基)硅丙基]四硫化物(BTSPS)和γ-缩水甘油醚丙基三甲氧基硅烷(GPTMS)复合硅烷化膜层.用反射吸收红外光谱、俄歇电子能谱(AES)和扫描电子显微镜(SEM)对复合膜层进行分析和表征.结果表明,在富含羟基氢氧化物的铝合金表面与BTSPS内膜层形成Al-O-Si共价键网络,BTSPS内层与GPTMS外层形成Si-O-Si共价键网络,环氧乙基位于复合膜层最外层.
参考文献
[1] | P. J. Herrera-Franco;A. Valadez-Gonzalez .Mechanical properties of continuous natural fibre-reinforced polymer composites[J].Composites. Part A, Applied science and manufacturing,2004(3):339-345. |
[2] | Kaynak C;Orgun O;Tincer T .Matrix and interface modification of short carbon fiber-reinforced epoxy[J].Polymer Testing,2005(4):455-462. |
[3] | R. E. Jensen;S. H. McKnight .Inorganic-organic fiber sizings for enhanced energy absorption in glass fiber-reinforced composites intended for structural applications[J].Composites science and technology,2006(3/4):509-521. |
[4] | A.J.Vreugdenhil;V.N.Balbyshev;M.S.Donley .Nanostructured Silicon Sol-Gel Surface Treatments for Al 2024-T3 Protection[J].JCT,2001(915):35-43. |
[5] | Tammy L M;Olga K;Edward T K .Spectroscopic and corrosion resistance characterization of GLYMO-TEOS Ormosil coatings for aluminum alloy corrosion inhibition[J].Progress in Organic Coatings,2002,44:295-305. |
[6] | 郭增昌,王云芳,王汝敏,熊艳丽.铝合金表面防腐蚀处理新工艺[J].材料保护,2005(04):25-27. |
[7] | Underhill P R;GoringG;DuQD .A study of the curing of 3-glycidoxypropyltrimethoxy silane films on aluminum[J].International Journal Adhesion & Adhesives,1998,18:313-317. |
[8] | Underhill P R;Goring G;Du Q D .A study of the deposition of 3-glycidoxypropyltrimethoxysilane on aluminum[J].International Journal Adhesion & Adhesives,1998,18:308-311. |
[9] | Underhill PR.;DuQuesnay DL.;Goring G. .The drying of 3-glycidoxypropyltrimethoxy silane[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,1998(1/4):247-253. |
[10] | O.Lunder;F.Lapique;B.Johnsen;K.Nisancioglu .Effect of pre-treatment on the durability of epoxy-bonded AA6060 aluminium joints[J].International Journal of Adhesion & Adhesives,2004(2):107-117. |
[11] | J.P.Sargent .Durability studies for aerospace applications using peel and wedge tests[J].International Journal of Adhesion & Adhesives,2005(3):247-256. |
[12] | Johnsen B B;Lapique F;Bjorgumb A et al.The effect of pre-bond moisture on epoxy-bonded sulphuric acid anodised aluminium[J].International Journal of Adhesion and Adhesives,2004,24:183-191. |
[13] | Lunder O;Olsen B;Nisancioglu K .Pre-treatment of AA6060 aluminium alloy for adhesive bonding International[J].Journal of Adhesion & Adhesives,2002,22:143-150. |
[14] | Maelund A;Rittenhouse J R;Labar W et al.Infrared reflection-absorption spectra of anodic oxide films on aluminum[J].Thin Solid Films,1974,21(01):67-72. |
[15] | Stralin A;Hjertberg T .Influence of surface composition on initial hydration of aluminium in boiling water[J].Applied Surface Science,1994,74:263-275. |