对MoSi2及其复相材料在高温、长时间老化后表面玻璃膜结构进行了研究.并用电学测试手段对表面玻璃膜的生成过程进行跟踪测试,以研究各复相材料表面玻璃膜的生成速度及机理.实验工作研究了MoSi2及MoSi2/SiC的氧化机理.氧化速度顺序为MoSi2>MoSi2/SiC.对于复相材料来讲,其玻璃膜的生成速度顺序为MS>MSM>MSA.
参考文献
[1] | Lin Wen .Silicon carbide and molybdenum silicide[J].Journal of the American Ceramic Society,1994,77(05):1162-1168. |
[2] | Maloy S A;Hener A H .Carbon additions to MoSi2 improved mechanical properties of molybdenum disilicide[J].Journal of the American Ceramic Society,1991,74(10):2704-2706. |
[3] | Jacobson N S;lee K N;Fox D S .Reactions of silicon carbide and silicon oxide at elevated temperatrures[J].Journal of the American Ceramic Society,1992,75(06):1603. |
[4] | Padrasta U;Ramamurty .Effect of carbon addition on elevated temperature crack growth resistance in MoSi2-SiC composite[J].Journal of American Ceramic Society,1994,77(10):2681-2688. |