本文以乙二胺作添加剂,采用溶胶-凝胶法制备了Y3+掺杂的纳米TiO2粉体.透射电镜TEM)分析结果表明,所制备的TiO2粉体具有纳米棒状结构,平均颗粒直径为15nm左右,长度为150~250nm左右.光催化降解硝基苯的实验结果说明,与盐酸作添加剂制备的TiO2粉体相比,乙二胺法制备的掺Y3+TiO2粉体具有更高的光催化降解性能.
参考文献
[1] | Fujishima A;Honda K .Electrochemical photolysis of water at a semiconductor electrode[J].Nature,1972,238:35-37. |
[2] | Frank S N;Bard A J .Heterogeneows photocatolytic oxidation of cyanide and sulfite in aqueous solutions at semiconductor powders[J].American Journal of Chemical Soc,1977,99:1484-1488. |
[3] | Matthew R W .Photooxidation of organic impurities in water using thin films of titanium dioxide[J].Journal of Physical Chemistry,1987,91(12):3328-3333. |
[4] | Matthew R W .Photo-oxidation of organic material in aqueous suspensions of titanium dioxide[J].Water Research,1986,20:569-578. |
[5] | 李慧泉,周新木.稀土掺杂二氧化态光催化的研究进展[J].江西化工,2003(02):13-15. |
[6] | Jun L;J immy Y C .Aninvestigation on photocatalytic activities of mixed TiO2 rare earth oxides for the oxidation of acetone in air[J].Journal of Photochemistry and Photobiology A:Chemistry,1998,116:63-67. |
[7] | 岳林海 .稀土元素掺杂二氧化钛催化剂光降解久效磷的研究[J].上海环境科学,1998,17(09):17-19. |
[8] | 周武艺,唐绍裘,张世英,周锡荣,万隆.制备不同稀土掺杂的纳米氧化钛光催化剂及其光催化活性[J].硅酸盐学报,2004(10):1203-1208. |
[9] | 高濂;郑珊;张青红.纳米氧化钛光催化材料及应用[M].北京:化学工业出版社,2002 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%