对日本耐火材料行业的总体现状和研究发展趋势进行了简要介绍与分析,就我国耐火材料行业发展中存在的问题提出了几点建议.

参考文献

[1] 马兴亚.日本近五十年钢铁冶炼耐火材料的进步[J].国外耐火材料,1997(05):3-6.
[2] Sugita K.The environmental problems of refractory—The discussed of Japan' s historical conditions.The International Refractory Technology[A].Orlando,United States,2005:104-114.
[3] Sugita K .An introduction to " the age of eco-refractories" -discussion of industrial furnaces and global environmental issues,based on a historical review[J].Industrial Heating,2008,45(04):52-63.
[4] 李庭寿,于景坤.日本耐火材料的技术现状及发展趋势[J].耐火材料,2002(03):171-174.
[5] 李少飞.日本不定形耐火材料现状[J].国外耐火材料,2006(03):4-9.
[6] 彭艳,谢朝晖.日本浇注料技术的最新进展[J].国外耐火材料,2006(05):1-5.
[7] 任敬文 .日本耐火材料工业的发展[J].耐火材料,2002,36(02):122-123.
[8] Torigoe A;Inoue K;Hoshiynma Y .Improvement of spalling resistance of low carbon MgO-C bricks[J].J Tech Assoc Refract,2004,56(06):278-281.
[9] 杜涛,蔡九菊,李亚军,王建军.炼铁-炼钢界面温降与节能模式分析[J].钢铁,2008(12):83-86,91.
[10] Takanaga S;Ochiai T;Tamura S.The application of the nano structural matrix to MgO-C bricks[A].Osaka,Japan,2003:521-524.
[11] Shiratani Y;Yotabun T;Chihara K.The Application of the nano structual matrix to SN plates[A].Orlando,United States,2005:575-578.
[12] Hattanda H;Yotabun T;Tsuda T.Application of nano structured matrix to SN plates[A].Dresden,Germany,2007:204-207.
[13] Yasumitsu H;Hirashima M;Matsuura O.The basic study on the formation of the nano structured marix in MgO-C bricks[A].Kyoto,Japan,2011:2-E-17.
[14] Tanaka M;Kamio H;Yoshitomi J.Nano-tech.MgO-C bricks for converters to minimize the heat loss[A].Kyoto,Japan,2011:2-E-18.
[15] Tamura S;Ochiai T;Takanaga S.Technological philosophy and evolution of nano-tech.refractories[A].Kyoto,Japan,2011:2-E-16.
[16] Tamura S;Ochisi T;Takanaga S.Nanoteeh refractories(Ⅰ)-The development of the nano structural matrix[A].Osaka,Japan,2003:517-520.
[17] Matsui T;Goto K;Yamada Y.Charteristics and application of nanotech magnesia carbon bricks[A].Orlando(USA),2005:176-179.
[18] Tamura S;Ochisi T;Matsui T.Technological Philosophy and Perspective of Nanotech Refractories[J].NIPPON STEEL TECHNICAL REPORT,2008(98):18-28.
[19] Fujiwara Y;Namba K;Takanaga S .Development of nano-tech MgO-C bricks(Ⅰ)-Effect of nano-structural matrix[J].Refractories,2004,56(03):120.
[20] Fujiwara Y;Namba K;Takanaga S .Development of nano-tech MgO-C bricks(Ⅰ)-Applycation of nano-structural matrix[J].J Tech Assoc Refract Jpn,2004,24(03):210.
[21] Dohke M;Nanba K;Takanaga S .Development of nano-tech MgO-C bricks " MgO-rimmed MgO-C brick"[J].Refractories,2004,56(03):121.
[22] MAYUKO DOHKE;KATSUSHIGE NAMBA;SHIGEYUKITAKANAGA .Development of Nano Tech MgO-C Brick (2) "Magnesia-rimmed MgO-C Brick"[J].Journal of the Technical Association of Refractories,2004(3):211-0.
[23] Hatta M;Nanba K;Takanaga S .Development of nano-tech MgO-C brick (Ⅲ) -Nano-structrue matrix MgO-C bricks[J].Refractories,2004,56(03):122.
[24] MANABU HATTA;KATSUSHIGE NAMBA;SHIGEYUKI TAKANAGA .Development of Nano Tech MgO-C Brick (3) "MgO-C Brick with Nano Structural Matrix"[J].Journal of the Technical Association of Refractories,2004(3):212-0.
[25] 廖文(编译).新日铁耐火材料发展评述[J].冶金管理,2010(09):58-60.
[26] 廖建国,桂明玺.水泥回转窑用碱性砖无铬化的状况[J].国外耐火材料,2004(03):1-7.
[27] 廖建国.水泥回转窑用无铬砖的演变[J].国外耐火材料,2003(05):6-10.
[28] 桂明玺.焚烧炉用喷涂料的现状[J].国外耐火材料,2004(02):6-9,32.
[29] 周雅坤.旭硝子公司--全球发展战略和经营改革[J].国际化工信息,2002(09):20-23.
[30] 西村雅史;佐々木久晴;難波誠 .取鍋用流し込み材の軽量化についての検討[J].耐火物,2010(1):28-29.
[31] 加藤田一平;生田良三 .ノンファイバー低熱伝導キャスタブルの実炉への適用[J].耐火物,2009(2):98-99.
[32] 加藤田一平;生田良三 .セメン卜製造におけるノンファイバー低熟伝導キャス夕ブルの展開[J].耐火物,2009(7):348-349.