介绍了非氧化物多孔陶瓷的制备方法、原理、工艺及其特点,综述了单相非氧化物(包括SiC、Si3 N4、SiAlON、TiB2、TiN、Ti3 SiC2和Ti3 AlC2)及SiC、Si3 N4和TiB2基复合多孔陶瓷的研究新进展,并展望了非氧化物多孔陶瓷的发展方向。

The preparation methods,principles,technology and the characteristics of non-oxide porous ce-ramics were introduced,and the latest progress of single phase non-oxides (including SiC,Si3 N4,SiAlON, TiB2,TiN,Ti3SiC2,and Ti3AlC2)and SiC based,Si3N4 based and TiB2 based composite porous ceramics were reviewed.The development trend of non-oxide porous ceramics was prospected.

参考文献

[1] Ren Fengzhang;Wang Zhe;Ma Zhanhong;Su Juanhua;Li Fengjun;Wang Limei.Effects of Fe_2O_3 concentration on microstructuresand properties of SiC-based ceramic foams[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,20091/2(1/2):113-116.
[2] Liu, G.;Dai, P.;Wang, Y.;Yang, J.;Qiao, G..Fabrication of pure SiC ceramic foams using SiO_2 as a foaming agent via high-temperature recrystallization[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,20116(6):2418-2422.
[3] 王慧;曾令可;张海文;罗民华;张明;程小苏;史琳琳;陈永洁.多孔陶瓷--绿色功能材料[J].中国陶瓷,2002(3):6-8,19.
[4] 吴海波;袁波;韩建燊;王刚.多孔陶瓷材料的制备研究进展[J].耐火材料,2012(3):230-235.
[5] Yong Li;Fei Chen;Ling Li;Weiru Zhang;Honglin Yu;Yubo Shan;Qiang Shen;Hongyi Jiang.Gas Pressure Sintering of Arbitrary Porous Silicon Nitride Ceramics with High Mechanical Strength[J].Journal of the American Ceramic Society,20106(6):1565-1568.
[6] Xiaowei Yin;Xiangming Li;Litong Zhang.Microstructure and Mechanical Properties of Lu2O3-Doped Porous Silicon Nitride Ceramics Using Phenolic Resin as Pore-Forming Agent[J].International journal of applied ceramic technology,20103(3):391-399.
[7] 赵毅;朱振峰;贺瑞华;胡俊涛.多孔陶瓷材料的的研究现状及应用[J].陶瓷,2008(7):27-30.
[8] 朱小龙;苏雪筠.多孔陶瓷材料[J].中国陶瓷,2000(4):36-39.
[9] 杨尔慧;王俊勃;姜凤阳;思芳.牺牲模板法制备多孔陶瓷材料的研究进展[J].电子元件与材料,2015(8):5-8,25.
[10] Studart, AR;Gonzenbach, UT;Tervoort, E;Gauckler, LJ.Processing routes to macroporous ceramics: A review[J].Journal of the American Ceramic Society,20066(6):1771-1789.
[11] 韩少维 .TiB<,2>多孔陶瓷的制备研究[D].武汉理工大学,2007.
[12] 刘岗;严岩.冷冻干燥法制备多孔陶瓷研究进展[J].无机材料学报,2014(06):571-583.
[13] 刘波涛;骆兵;许壮志;刘贵山.冷冻浇注成型多孔陶瓷的研究进展[J].中国陶瓷,2010(11):7-11.
[14] Annemarie Preiss;Bo Su;Simon Collins.Tailored graded pore structure in zirconia toughened alumina ceramics using double-side cooling freeze casting[J].Journal of the European Ceramic Society,20128(8):1575-1583.
[15] 吴海波;袁波;韩建燊;王刚.凝胶注模常温发泡制备氧化铝多孔陶瓷[J].材料科学与工艺,2012(04):144-148.
[16] 朱振峰;杨冬;刘辉;孙洪军;张建权;郭丽英.生物模板法制备多孔陶瓷的研究进展[J].材料导报,2009(21):50-54.
[17] Yang GB;Liu YJ;Qiao GJ;Yang JF;Wang HJ.Preparation and R-curve properties of laminated Si/SiC ceramics from paper[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,20081/2(1/2):327-332.
[18] S.A. Silva;D.D. Brunelli;F.C.L. Melo.Preparation of a reticulated ceramic using vegetal sponge as templating[J].CERAMICS INTERNATIONAL,20094(4):1575-1579.
[19] G. Amirthan;A. Udayakumar;V.V. Bhanu Prasad.Synthesis and characterization of Si/SiC ceramics prepared using cotton fabric[J].CERAMICS INTERNATIONAL,20093(3):967-973.
[20] C. X. F. Lam;X. M. Mo;S. H. Teoh;D. W. Hutmacher.Scaffold development using 3D printing with a starch-based polymer[J].Materials science & engineering, C. Biomimetic and supramolecular systems,20021/2(1/2):49-56.
[21] Seitz H;Rieder W;Irsen S;Leukers B;Tille C.Three-dimensional printing of porous ceramic scaffolds for bone tissue engineering.[J].Journal of biomedical materials research, Part B. Applied biomaterials,20052(2):782-788.
[22] 邓先功;王军凯;杜爽;曹迎楠;李发亮;张海军;张少伟.发泡法、三维打印法、熔盐法制备多孔陶瓷[J].材料导报,2015(9):109-116.
[23] 黄仲;焦成鹏;张少伟;张海军;李发亮;鲁礼林.熔盐法合成非氧化物陶瓷粉体[J].耐火材料,2015(3):232-237.
[24] Shaowei Zhang;Yan Wen;Haijun Zhang.Low temperature preparation of tungsten nanoparticles from molten salt[J].Powder Technology: An International Journal on the Science and Technology of Wet and Dry Particulate Systems,2014:464-466.
[25] 陈以心;王日初;王小锋;彭超群;孙月花.多孔SiC陶瓷的研究进展[J].中国有色金属学报,2015(8):2146-2156.
[26] 于雪梅.气体静压轴承用多孔SiC陶瓷的制备及静态性能[J].西安交通大学学报,2011(03):117-120.
[27] 杨阳;赵宏生;刘中国;张凯红;李自强.烧结温度对包混/复合添加工艺制备多孔SiC陶瓷性能的影响[J].材料导报,2011(2):40-42.
[28] 徐慢;王亮;祝云;王树林;沈凡;季家友.多孔大通量莫来石相碳化硅陶瓷的制备与表征[J].武汉工程大学学报,2015(2):15-20.
[29] 李俊峰;林红;李建保.碳化硅多孔陶瓷气孔率和强度影响因素[J].无机材料学报,2011(9):944-948.
[30] 氮气压力对多孔氮化硅陶瓷显微组织和力学性能的影响[J].无机材料学报,2014(07):701-705.
[31] 王鹏举;吴玉萍;应国兵;田宝娜;王乘;李嘉;赵海伟.凝胶注模技术制备高强度多孔氮化硅陶瓷[J].硅酸盐学报,2014(12):1496-1500.
[32] 翁作海;曾庆丰;谢聪伟;彭军辉;张瑾.三维打印结合反应烧结制备多孔氮化硅陶瓷[J].材料导报,2013(8):5-7,10.
[33] 于方丽;于平平;王俭志;杨建锋.烧结助剂及β-Si3N4添加量对多孔氮化硅陶瓷性能的影响[J].人工晶体学报,2011(3):772-778,783.
[34] 鲁元;杨建锋;李京龙.碳热还原-反应烧结法制备多孔氮化硅陶瓷[J].无机材料学报,2013(5):469-473.
[35] 王涛;余娟丽;吕毅;郭世峰;裴雨辰.多孔Sialon陶瓷的冷冻凝胶法制备与表征[J].宇航材料工艺,2015(4):43-46.
[36] 王光 .B-SiAlON陶瓷及其多孔材料制备工艺研究[D].大连海事大学,2011.
[37] 韩少维;王为民;傅正义;王皓.放电等离子烧结法制备二硼化钛多孔陶瓷[J].稀有金属材料与工程,2007(z1):549-552.
[38] 鲁元;龚楠;荆强征;李京京;炱柯.碳热还原法制备多孔氮化钛陶瓷[J].陶瓷学报,2014(2):177-181.
[39] 王俊平 .凝胶注模成型硼化锆多孔陶瓷[D].安徽理工大学,2015.
[40] M. Fraczkiewicz;A.G. Zhou;M.W. Barsoum.Mechanical damping in porous Ti_3SiC_2[J].Acta materialia,200619(19):5261-5270.
[41] Shi SL;Pan W.Machinable Ti3SiC2/Hydroxyapatite bioceramic composites by spark plasma sintering[J].Journal of the American Ceramic Society,200710(10):3331-3333.
[42] Ziqi Sun;Meishuan Li;Longfei Hu.Surface Chemistry, Dispersion Behavior, and Slip Casting of Ti_3AlC_2 Suspensions[J].Journal of the American Ceramic Society,20098(8):1695-1702.
[43] 曹辉 .Ti3AlC2多孔陶瓷的制备及性能研究[D].北京交通大学,2015.
[44] 马战红;任凤章;赵培峰.添加剂对SiC-Al2O3陶瓷过滤器性能的影响[J].中国陶瓷,2009(8):21-23.
[45] 马永华;罗民;吕玉琴;丁肖怡;候广亚.冰模板法制备反应结合多孔Si3N4/SiC复相陶瓷[J].人工晶体学报,2014(8):1998-2005.
[46] 景亚妮;邓湘云;李建保;白成英;蒋文凯;李誉;刘张敏.SiC/莫来石复相多孔陶瓷气孔率和强度的影响因素[J].硅酸盐通报,2013(10):1979-1983.
[47] 李书海;崔洪芝;郑文龙;崔德运.SiCw对反应烧结多孔Al2TiO5-SiCw复合材料的影响[J].复合材料学报,2014(5):1270-1276.
[48] 何恩全;岳建设;王红洁;乔冠军.反应烧结制备多孔β-sialon/Si3N4陶瓷[J].硅酸盐学报,2010(8):1459-1462.
[49] 谢继峰;曹顺华;张秀芳;李文超.反应烧结制备多孔TiB2-TiC复相陶瓷[J].中国有色金属学报,2009(8):1468-1472.
[50] 韩超;曹顺华;刘慧远.原料B4C粉末粒度对多孔 TiB2-TiC复相陶瓷孔结构的影响[J].粉末冶金材料科学与工程,2011(5):678-681.
[51] 苏娟;钱东浩;周小新;张树格;徐升美.自蔓延高温合成多孔陶瓷(Al2O3-TiB2)的研究[J].粉末冶金技术,2006(1):24-28.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%