用热等离子弧在Q235钢基体表面熔覆材料为Stellite Ni60商用镍基自熔性合金粉的涂层,涂层厚1 mm.对熔覆层的耐蚀性能进行了研究,并对耐蚀机理进行分析,结果发现,熔覆层耐碱的腐蚀性最好,其次是耐食盐水腐蚀,耐盐酸的腐蚀性相对较差.
参考文献
[1] | Woodruff D P;Delchar T A.Modern Techniques of surface science[M].England:Cambridge University Press,1986:104. |
[2] | Atamert S;Mordasov V I .Comparison of the microstructure and abrasive wear properties of stellite hardfacing alloys deposited by arc welding and laser cladding[J].Metallur Trans,1989,20A:126. |
[3] | Wang Xibao;Liu Hua .Metal powder thermal behavior during the plasma transferred-arc surfacing process[J].Surface and Coatings Technology,1998,106:156-161. |
[4] | Hahn H .Gas synthesis of nanocrystalline materials[J].Nano-Structured Materials,1996,19(08):3-11. |
[5] | Li Q;Lei T C;Chen W Z .Microstructure characterization of laser-clad TiCp-reinforced Ni-Cr-B-Si-C composite coatings on steel[J].Surface and Coatings Technology,1999,114:278-284. |
[6] | 赵程,田丰,侯俊英.等离子弧金属表面熔覆处理的研究[J].金属热处理,2002(02):3-5. |
[7] | 田丰 .热等离子弧熔覆技术的研究[D].青岛科技大学,2002. |