以甲苯二异氰酸酯、聚醚多元醇、二羟甲基丙酸、1,4 丁二醇、甲基丙烯酸甲酯、甲基丙烯酸丁酯等为原料,采用原位乳液聚合工艺合成聚氨酯聚丙烯酸酯乳液.研究了单体含量对乳液及胶膜性能的影响.实验结果表明:随着乙烯基单体含量的增加,乳液稳定性下降;胶膜的断裂伸长率降低,硬度和耐水性增加.当乙烯基单体的质量分数为35%时,乳液的稳定性大于365 d,胶膜的断裂伸长率为482%,摆杆硬度为0.68,吸水率为18.7%.红外光谱分析表明合成了聚氨酯聚丙烯酸酯.
参考文献
[1] | Jung YC;Sahoo NG;Cho JW .Polymeric nanocomposites of polyurethane block copolymers and functionalized multi-walled carbon nanotubes as crosslinkers[J].Macromolecular rapid communications: Publishing the newsletters of the European Polymer Federation,2006(2):126-131. |
[2] | Kukanja D.;Zupancic-Valant A.;Krajnc M.;Golob J. .The structure and properties of acrylic-polyurethane hybrid emulsions and comparison with physical blends[J].Journal of Applied Polymer Science,2000(1):67-80. |
[3] | Manock H L .New developments in polyurethane and PU/acrylic dispersions[J].Pigment & Resin Technology,2000,29(03):143-151. |
[4] | 王春鹏,储富祥,金立维,林明涛,GUYOT Alain.不同端基聚氨酯-丙烯酸酯复合细乳液的表征[J].高分子材料科学与工程,2006(05):90-94. |