采用X-射线衍射、扫描电镜及能谱等测试手段,研究了一种镍基单晶合金在75% Na2SO4+25% K2SO4熔盐中的热腐蚀行为,该熔盐θ为900℃.结果表明,镍基单晶合金热腐蚀严重,出现严重的内硫化和内氧化;外层腐蚀产物由Al2O3 、Cr2O3 Ni2Cr2O4和Co2Cr2O4相组成,内层为Al2O3和CrS;镍基单晶合金表面形成的氧化物发生碱性溶解.
参考文献
[1] | Ren Xin;Wang Fu-hui;Wang Xin .High-temperature Oxidation and hot corrosion behaviours of the NiCr-CrAl coating on anickel-based superalloy[J].Surface and Coatings Technology,2005,198:425-426. |
[2] | Huang L;Sun X F;Guan H R et al.Oxidation behaviour of a sinagel-crystal Ni-base superalloy in air at 900,1000 and 1100 ℃[J].Tribology Letters,2006,23(01):15-16. |
[3] | Das S;Datta S;Basu D et al.Hot corrosion of galss coating on nickel based superalloy[J].Ceramica International,2008,34:1217-1218. |
[4] | 李维银,刘红飞,赵双群.新型镍基高温合金950℃氧化行为的研究[J].材料热处理学报,2008(03):26-29. |
[5] | Li M H;Sun X F;Hu W Y et al.Hot corrosion of a single crystal Ni-base superalloy by Na-salts at 900 ℃[J].Oxidation of Metals,2006,65(1/2):147-148. |
[6] | Ren X;Wang FH .High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing[J].Surface & Coatings Technology,2006(1/2):30-37. |
[7] | 赵双群,谢锡善.新型Ni-Cr-Co基高温合金的热腐蚀行为[J].材料科学与工艺,2006(05):506-509. |
[8] | 任鑫,王福会,汪信.Al-Si涂层在900℃硫酸盐中的热腐蚀行为[J].腐蚀科学与防护技术,2004(04):187-191. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%