综述了空间环境因素的特征及其效应,包括太阳电磁辐射、带电粒子辐射、空间真空效应、冷黑环境、原子氧侵蚀、微流星和空间碎片的撞击.碳(石墨)纤维、环氧树脂、碳(石墨)/环氧复合材料的性能以及碳(石墨)/环氧复合材料在航天器上的应用和研究现状.

参考文献

[1] 贾乃华.宇航物理[M].北京:科学出版社,1990:7-8.
[2] 王浚;黄本诚;万才大.环境模拟技术[M].北京:国防工业出版社,1996:214-217.
[3] 贺福;王茂章.碳纤维及其复合材料[M].北京:科学出版社,1997:175,273-277.
[4] 曾汉民.高技术新材料要览[M].北京:中国科学技术出版社,1993:21-27.
[5] 沃丁柱.复合材料大全[M].北京:化学工业出版社,2000:1060-1063.
[6] 高慎斌.卫星制造技术[M].北京:宇航出版社,1998:67-72.
[7] 沃西源;张惠丽;卢大成 .石墨/环氧卫星天线支撑结构研制与质量控制[J].宇航材料工艺,1997,4(04):47-51.
[8] 韩鸿硕 .国外航天运输系统防热系统、结构和材料的总体分析研究[J].宇航材料工艺,1997,4
[9] 邱惠中 等.国外航天材料的新进展[J].宇航材料工艺,1997,4(04)
[10] 甄华生 .复合材料在航天器中的应用近况[J].宇航材料工艺,1997,4:14-16.
[11] 江辉 .国外航天结构新材料发展简述[J].宇航材料工艺,1998,4(04):1-8.
[12] Rutledge Sharon K;Paulsen Phillip E;Brady Joyce A .Evaluation of Atomic Oxygen Resistant Protective Coatings for Fiberglass-Epoxy Composites in LEO[R].NASA N89-21100
[13] Stein Bland A;Pippin Gary H .Preliminary Findings of the[Z].
[14] Bourassa R J;Gillis J R;Rousslang K W .Atomic Oxygen andUltraviolet Radiation Mission Total Exposures for LDEF Experiments[P].NASA N92-24808
[15] Tennyson R C;Mabson G E;Morison W D;Kleiman J .Preliminary Results From The LDEF/UTIAS Composite Materials Experiment[R].NASA N92-24837
[16] Felbeck D K .High-Toughness Graphite/Epoxy Composite Material Experiment[R].NASA N92-24841
[17] Slemp Wayne S;Young Philip R;Witte William G .Effectsof LDEF Flight Exposure on Selected Polymer Matrix ResinComposite Materials[P].NASA N92-24842
[18] Heinrich JABS .Effect of Space Exposure of Some Epoxy Matrix Composites on Their Thermal Expansion and MechanicalProperty[R].NASA N92-24844
[19] Tennyson R C;Matthews R .Themal-Vacuum Response ofPolymer Matrix Composites in Space[R].NASA N94-31033
[20] Jang Bor Z;Bianchi J;LIU Y M .Space Environmental Effects on Polymer Composites: Research Needs and Opportuntties[R].NASA N94-31035
[21] George Pete E .Low-Earth Effects on Organic Composite Materials Flown on LDEF[P].NASAN94-31036
[22] Grammer Holly;Wightman James p .Surface Characterization of LDEF Carbon Fiber/Polymer Matrix Composites[P].NASA N95-23900
[23] Harry Dursch;Pete George .Organic Matrix Composite Protective Coatings for Space Applications[P].NASA N95-23914
[24] Startsev Oleg V .Structure and Properties of Polymeric Composite Materials During 1501 Days Outer Space Exposure at"Salyut-7” Orbital Station[P].NASA N95-23915
[25] ВарбашевЕА;лущинМИ.Некоторыереэльтатыиснытанийноли4мерныхматериалоннослеэкснониронаниянуслонияхоткрытогокосмоса. госмическаятехнологияиматериалонедение[J].ИздательстноНаука Москва,1982:78-82.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%