欢迎登录材料期刊网

材料期刊网

高级检索

介绍了一种网格结构用橡胶模具的研究.所研制出的硅橡胶配方的拉伸强度为1.11MPa,断裂伸长率为95.6%,比热容为2.068×103J/(kg*K),导热系数为0.224W/(m*K),密度为1.087×103 kg/m3,线收缩率为1.05%,邵氏硬度为60.该配方具有良好的成型工艺性.并利用该配方成功的制作出了φ480网格结构缠绕成型用模具.

参考文献

[1] 于翘.材料工艺[M].北京:宇航出版社,1993:276-278.
[2] KOURY J L;KIM T D;TRACY J J;HARVEY J A.Continuous fiber composite isogrid structure for space applications.Proceedings of the 1993 conference on processing,fabrication and applications of advanced composites[A].Long beach,CA,9-11,1993:193-197.
[3] HUYBRECHTS S;MEINK T E.Advanced grid stiffened structures for the next generation of launch vehicles[A].Piscataway, NJ, Institute of Electrical and Electronics Engineers, Inc,1997:263-270.
[4] VASILIEV V V;BARYNIN V A;RASIN A F.Anisogrid lattice structures-survey of development and application[J].Computers and Structures,2001(54):361-370.
[5] 陆集平.碳/环氧复合材料网格加筋结构的研制[A].,1988:1131-1136.
[6] 章基凯.有机硅材料[M].北京:中国物资出版社,1999:275-276.
[7] 幸松民;王一璐.有机硅合成工艺及产品应用[M].北京:化学工业出版社,2000:634-643.
[8] 郭亚林,梁国正,丘哲明,冯喜利,成敏苏.纳米SiOx改性室温硫化硅橡胶研究[J].弹性体,2003(01):19-22.