综述了在污染大气环境中金属材料初期腐蚀行为和机理研究进展.目前主要采用的研究方法包括试验方法(室外暴露试验、室内加速试验)、检测方法(腐蚀速率的测定、腐蚀产物的分析和表面形貌的观察)和电化学监测方法,用原位动态实时监测技术来研究初期腐蚀机理是重点发展的方向.重点阐述了单个或混合污染物对几种典型金属材料(铜、锌、钢等)初期腐蚀行为的影响和作用的研究情况.

参考文献

[1] 王光雍,王海江,李兴濂等编著.自然环境的腐蚀与防护-大气·海水·土壤[M].北京:化学工业出版社,1997.
[2] 托马晓夫著.金属腐蚀及其保护的理论[M].北京:中国工业出版社,1964.
[3] Damian L and Fako R. Weathering structural corrosion in atmospheric of various degrees of pollution in romania[J ]. Mate-rials and Corrosion, 2000, 51 (8) :574.
[4] Johansson L - G and Vannerberg N - G. The atmospheric corrosion of unprotected carbon steel - A comparison between field study and laboratory test[J ]. Werkstoffe Und Korrosion,1981, 32:265.
[5] Eriksson P, Johansson L - G and Strandberg H. Initial stages of copper corrosion in humid air containing SO2 and NO2 [J ].Journal of Eletrochemical Society, 1993, 140(1):53.
[6] Aastrup T, Wadsak M, Schreiner M, et al. Experimental in situ studies of copper exposed to humidified air[J]. Corrosion Science, 2000, 42: 957.
[7] Wadsak M, Schreiner M, Aastrup T, et al. Combined in - situ investigations of atmospheric corrosion of copper with SFM and IRAS coupled with QCM[J]. Surface Science, 2000, 454- 456:246.
[8] 严川伟,曹楚南,林海潮.石英晶体微天平(QCM)在大气腐蚀研究中的应用[J].中国腐蚀与防护学报,2001,21(2):123.
[9] 王凤平,严川伟,张学元,等.石英晶体微天平(QCM)及其在大气腐蚀研究中的应用[J].化学通报,2001,(6):382-387.
[10] 王风平,严川伟,张学元.石英昌体微天平研究Zn在薄液膜下的腐蚀动力学[J].物理化学学报,2001,17(4):319-323
[11] 张学元,韩恩厚,PerssonD,等.利用1RAS研究锌表在在湿干交替条件下的腐蚀行为[J].中国腐蚀与防护学报,2002,22(1):32.
[12] Sziraki, Szocs E, Pilbath Z, et al. Study of the white rust formation on zinc single crystal by EIS/AFM and SEM/EDS techniques[ J ]. Electrochimica Acta, 2001,46: 3743.
[13] Chung S C, Liou Y M, Shiu M S, et al. EXAFS study of atmospheric corrosion products on zinc at the initial stage[J ]. Corrosion Prevention and Control, 1999, 12:163.
[14] Dean S W. Planning, instrumentation, and evalution of atmospheric corrosion tests(Part 4) [ J ]. Environment Treatment & Control, 1989, (1) :52.
[15] Pacheco A M G, Teixeira M G I B and Ferreira M G S. Initial stages of chloride induced atmospheric corrosion of iron: An Infrared Spectroscopic Study [ J ]. British Corrosion Journal,1990, 25(1) :57.
[16] Nishikata A, Ichihara Y, Hayashi Y, et al. Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron [ J ]. Journal of Eletrochemical Society,1997, 144(4): 1244.
[17] Quintana P, Veleva L, Cauich W, et al. Study of composition and morphology o[ initial stage of corrosion products formed on Zn plates exposed to the atmosphere of southeast mexico[J ]. Applied Surface Science, 1996, 99: 325.
[18] Odnevall I. Doctoral Thesis. Atmospheric corrosion of field exposed zinc - A multianalytical characterisation of corrosion products from initial films to fully developed layers[J ]. RoyalInstitute of Technology, Sweden, 1994.
[19] Almeida E. Atmospheric corrosion of Zinc part 1; Rural and Urban Atmospheres [ J ]. British Corrosion Journal, 2000, 35(4):284.
[20] Almeida E. Atmospheric corrosion of Zinc part l:Marine atmospheres[J ]. British Corrosion Journal, 2000, 35(4) :289.
[21] Odnevall I and Leygraf C. Formation of Zn2SO4(OH)6·4H2O in a rural atmosphere [ J ]. Corrosion Science, 1994, 36 ( 6 ):1077.
[22] Odnevall I and Leygraf C. Formation of NaZn2Cl(OH)6SO4· 6H2O in marine atmosphere [ J ]. Corrosion Science, 1993, 34(7): 1213 - 1229.
[23] Svensson J - E and Johansson L - G. A laboratory study of the initial stages of the atmospheric corrosion of Zinc in the presenceof NaCl: Influence of SO2 and NO2 [J]. Corrosion Science, 1993, 34(5) :721.
[24] Qing Qu, Chuanwei Yan, Ye Wan, et al. Effects of NaCl and S5O2 on the initial atmospheric corrosion of Zinx[J ]. Corrosion,2002, 44:2789.
[25] Neufeld A K, Cole I S, Bond A M, et al. The initial mechanism of corrosion of Zinc by sodium chloride particle deposition[J ]. Corrosion Science, 2002, 44: 555.
[26] Chawla S K and Payer J H. The early stage of atmospheric corrosion of copper by sulfur dioxide [J ]. Journal of Eletrochemical Society, 1990, 137(1) :60.
[27] Itoh J, Sasaki T, Seo M, et al. In situ simultaneous measurement with IR - RAS and QCM for corrosion of copper in a gaseous environment [ J ]. Corrosion Science, 1997, 39 ( 1 ):193.
[28] Wadsak M, Aastrup T, Odnevall I, et al. Multianalytical of situ investigation of the initial atmospheric corrosion of bronze[J ].Corrosion Science, 2002, 44: 791.
[29] Eriksson P, Johansson L - G and Strandberg H. Experimental in situ studies of copper exposed to humidified air[J ]. Journal of the Eletrochemical Society, 1993,140( 1 ): 53.
[30] Eriksson P, Johansson L - G and Gullman J. A laboratory study of corrosion reactions on statue bronze [ J ]. Corrosion Science, 1993, 34(7): 1083.
[31] Aastrup T, Wadsak M, Leygraf C and Schrenner M. In situ studies of the initial atmospheric corrosion of copper-Influence of humidity, sulfur dioxide, ozone, and nitrogen dioxide [ J ].Journal of the Eletrochemical Society, 2000, 147(7): 2543.
[32] Persson D and Leygraf C. In situ infrared reflection absorption spectroscopy for studies of atmospheric corrosion [J ]. Journal of the Eletrochemical Society, 1993, 140(5) :1256.
[33] 曾小勤,王渠东,吕宜振,等.镁合金应用新进展[J].铸造,1998,11:39.
[34] 刘正,王越,王光中,等.镁基轻质材料的研究与应用[J].材料研究学报,2000,14(5):449.
[35] 杨彬.镁合金研究及制备发展情况[J].铸造设备研究,2001, 1:36.
[36] E M Gutman, A Eliezer, Ya Unigovski, et al. Corrosioin and protection of magnesium alloys[J ]. Material Science and Engineering, 2001, A302: 63.
[37] 吴振宁,李培杰,刘树勋,等.镁合金腐蚀问题研究现状[¨.铸造,2002,50(10):583.
[38] 许越,陈湘,吕祖舜,等.镁合金表面的腐蚀特性及其防护技术[J].哈尔滨工业大学学报,2001,33(6):753.
[39] Lindstrom R, Svensson J - E and Johansson L - G. The influence of carbon dioxide on the atmospheric corrosion of some magnesium alloys in the presence of NaCl [ J ]. Journal of the Eletrochemical Society, 2002, 149(4) :B103.
[40] Zakipour S, Laygraf C and Portnoff G. Studies of corrosion kinetics on electrical contact materials by means of QCM and XPS[J].Journal of the Eletrochemical Society, 1986, 133(5) :873.
[41] Tidblad J and Graedel T E. GI LDES model studies of aqueous chemistry Ⅳ. Initial (NH4)2SO4-induced atmospheric corrosion of copper[J ]. Journal of Eletrochemical Society, 1997, 144(8):2676.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%