介绍了四种体积型腐蚀缺陷的评价方法,对比分析了其特点及适用性.结论为:ANSI/ASME-B31G适用于管材等级较低、管道服役年限长的老管道的评估,半经验、偏保守;DNV法可进行单个缺陷、相互作用的缺陷和复杂形状缺陷的评估;SY/T6151-1995法评价过程较复杂,但评价结果较准确;API RP 579-2000是目前较先进、较精确的分级评估方法,我国的SY/T6477-2000等效于它.

参考文献

[1] ANSI/ASME B31G,Manual for Determining the Remaining Strength of Corroded Pipelines[S].America,1991.
[2] CAN/CSA Z184 -M86 -1986,Gas Pipeline Systems[S].Canada,1986.
[3] DNV RP F101 -1999,Corroded Pipelines[S].Norway,1999.
[4] API 579,Recommended Practice for Fitness-for-service[S].America,2000.
[5] SY/T 6151-1995,钢质管道管体腐蚀损伤评价方法[S].1995.
[6] SY/T 6477-2000,含缺陷油气输送管道剩余强度评价方法[S].2000.
[7] Central Electricity Generating Board(CEGB) R/H/R6-Revision 3.Assessment of the Integrity of Structure Containing Defects[S].UK,1986.
[8] 严大凡,翁永基,董绍华.油气长输管线风险评价与完整性管理[M].北京:化学工业出版社,2005.72.
[9] K E W Coulson,R G Worthingham.Standard damage assessment approach is overly conservative[J].Oil and Gas Journal,1990,(9):54.
[10] T J O′Grade,D T Hisey,J F Kiefner.Method for evaluating corroded pipe addresses variety of patterns[J].Oil and Gas Journal,1992,(12):77.
[11] 张建礼,王克强,陈建民.东黄老线剩余强度评价[J].油气储运,2000,19(9):46.
[12] 姜晓红,李力耘,付桂英.管道缺陷评估方法[J].油气储运,2005,24(增刊):52.
[13] 刘海峰,王毅辉.在役油气压力管道腐蚀剩余强度评价方法探讨[J].天然气工业,2001,21(6):90.
[14] 赵新伟,李鹤林.油气管道完整性管理技术及其进展[J].中国安全科学学报,2006:16(1)129.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%