通过系列热处理和热充氧实验,采用光学显微镜、SEM和拉伸试验等研究了不同温度时效处理对沉淀硬化马氏体不锈钢FV520B的氢脆敏感性的影响.结果表明:充氢后,FV520B钢表现出良好的抗氧脆件能;450℃低温时效后钢的氢脆敏感件较高,而630℃中温时效后,钢中由于析出较多的逆变奥氏体,阻碍氧扩散和裂纹扩展;充氢后表现出良好的抗氢脆性能.塑性损减率随钢中逆变奥氏体的增加而降低.

参考文献

[1] M Abdelshehid,K Mahmodieh,K Mori,et al.On the correlation between fracture toughness and precipitation hardening heat treatments in 15-5PH Stainless Steel[J].Engineering Failure Analysis,2007,14:626.
[2] A Perujo,F Serra,S Alberici,et al.Hydrogen in the martensitic DIN 1.4914:a review[J].Journal of Alloys and Compounds,1997,253-254:152.
[3] M Beghini,G Benamati,L Bertini,et al.Effect of hydrogen on the ductility reduction of F82H martensitic steel after different heat treatments[J].Journal of Nuclear Materials,2001,288:1.
[4] J M Hyzak,R E Stoltz.Hydrogen compatibility of HT-9 martensitic stainless steel[J].Journal of Nuclear Materials,1981,103/104:877.
[5] 刘中豪,陈廉.含氢马氏体时效钢低温力学性能行为与断裂机制[J].金属学报,1990,26:284.
[6] R B Hutchings,A Turnbull.The effect of prior mechanical deformation on hydrogen transport through 13% Chromium martensitic stainless steel[J].Corrosion Science.1992,33:713.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%