综述了CO2/H2S共存条件下的腐蚀机理、其影响因素和国内外CO2/H2S腐蚀的研究现状与趋势,提出了CO2/H2S共存时的选材要求及原则,展望了对CO2/H2S腐蚀的研究重点和抗CO2/H2S腐蚀钢的研发方向.

The corrosion mechanism of pipelines induced by muti-phase flow under the condition of CO2 and H2S coexistence and the main factors influencing corrosion process are discussed. Present researches and developments on CO2/H2Sinduced corrosion are reviewed. The demands and principles for material selection under CO2/H2S coexistence conditions are presented. The emphases trend of researches on CO2/H2S corrosion and CO2/H2S-corrosion resisting pipeline steels are also prospected.

参考文献

[1] Bolmer P W.Polarization of iron in H2S-NariS buffer[J].Corrosion,1965,21 (3):69.
[2] 白真权,李鹤林,刘道新,等.模拟油田H2S/CO2环境中N80钢的腐蚀及影响因素研究[J].材料保护,2003,36(4):32.
[3] Pots B F M,John R C.Improvement on De Wanrd-Milliams corrosion prediction and application to corrosion management[J].Corrosion/2002.Houston:NACE,2002,Paper No.02235.
[4] Agrawal A K,Durr C,Koch G H.Sulfide films and corrosion rates of AISI1018 carbon steel in saline solutions in the presence of H2S and CO2 at temperature up to 175°F[J].Corrosion/2004.Houston:NACE,2004,Paper No.04383.
[5] Kvarekval J,Nyborg R,Seiersten M.Corrosion product films on carbon steel in semi-sour CO2/H2S environments[J].Corrosion/2002.Houston:NACE,2002,Paper No.02296.
[6] Hausler R H,Stegman D W,Tjandroso D.Parametric study on the effect of H2S,condensate,metallurgy,and flowrate[J].Corrosion/1990.Houston:NACE,1990,Paper No.6.
[7] Smith S N,Paeheco J L.Prediction of corrosion in slightly sour environments[J].Corrosiou/2002.Houston:NACE,2002,Paper No.02241.
[8] 姜放,戴海黔,曹小燕.等.油套管在CO2和H2S共存时的腐蚀机理研究[J].石油与天然气化工,2005,34(3):213.
[9] Dagstad A.Mechanism of protective film formation during CO2 corrosion of carbon steel[J].Corrosion/1998[C].Houston:NACE,1998,Paper No.31.
[10] Hunnik E W J V,Pots B F M,Hendriksen E L J A,et al.The formation of protective FeCO3 corrosion product layers in CO2 corrosion[J].Corrosion/1996.Houston:NACE,1996,Paper No.6.
[11] Nyborg R.Initiation and growth of mesa corrosion attack during CO2 corrosion of carbon steel[J].Corrosion/1998.Houston:NACE,1998,Paper No.48.
[12] Kvarekval J,Nyborg R,Choi H,et al.Formation of muhilayer iron sulfide films during high temperature CO2/H2S corrosion of carbon steel[J].Corrosion/2003.Houston:NACE,2003,Paper No.03339.
[13] Ueda M.Effect of alloying elements and microstructure on stability of corrosion product in CO2 and/or H2S environments[J].Chemical Engineering of Oil and Gas,2005,34(1):43.
[14] Smith J S,Miller J D A.Nature of sulfides and their corrosive effect on ferrous metals[J].A Review,British Corrosion Journal,1975,10(3):136.
[15] Morse J W,Millero F J,Corowell J C,et al.The chemistry of the hydrogen sulfide and iron sulfide systems in natural waters[J].Earth-Science Reviews,1987,24 (1):1.
[16] Sun W,Nesic S,Papavinasam S.Kinetics of iron sulfide and mixed iron sulfide/carbonate scale precipitation in CO2/H2S corrosion[J].Corrosion/2006.Houston:NACE,2006,Paper No.06644
[17] 白真权,任呈强,刘道新.N80钢在CO2/H2S高温高压环境中的腐蚀行为[J].石油机械,2004,32(12):16.
[18] 李萍.90℃时油管钢P110的CO2/H2S腐蚀行为[J].全面腐蚀控制,2006,20(2):23.
[19] Brown B,Parakala S R,Nesic S.CO2 corrosion in the presence of trace amounts of H2S[J].Corrosion/2004.Honston:NACE,2004,Paper No.04736.
[20] 《油气田腐蚀与防护技术手册》编委会.油气田腐蚀与防护技术手册(下册)[M].北京:石油工业出版社,1999.471.
[21] Ramanarayanan T A,Smith S N.Corrosion of iron in gaseous environments and in gas-saturated aqueous environments[J].Corrosion,1990,46(1):66.
[22] 张清,李全安,文九巴,等.CO2分压对油管钢CO2/H2S腐蚀的影响[J].钢铁研究学报,2004,16(4):72.
[23] 周计明.油管钢在含CO2/H2S高温高压水介质中的腐蚀行为及防护技术的作用[D].西安:西北工业大学,2002.28.
[24] Mora-Mendoza J L,Chacon-Nava J G,Zavala-Olivares G,et al.Influence of turbulent flow on the localized corrosion processes of mild steel with inhibited aqueous CO2 systems[J].Corrosion,2002,58 (7):608.
[25] Abayarathna D,Naraghi A,Wang S H.The effect of surface films on corrosion of carbon steel in a CO2-H2S-H2O System[J].Corrosion/2005.Houston:NACE,2005,Paper No.05624.
[26] Ikeda A,Ueda M,Mukai S,et al.Influence of environmental factors on corrosion in CO2 source well[J].Corrosion/1985.Houston:NACE,paper No 29.
[27] 李国敏.碳钢在含硫化氧及高压二氧化碳饱和的NaCl溶液中的腐蚀行为[J].中国腐蚀与防护学报,2000,20(4):204.
[28] 张学元,邸超,雷良才.二氧化碳腐蚀与控制[M].北京:化学工业出版社,2000.15.
[29] Dugstad A,Lunde L.Parametric study of CO2 corrosion of carbon steel[J].Corrosion/1994.Honston:NACE,1994,Paper No.94014.
[30] Bich N N,Goerz K.Caroline pipeline failure:Findings on corrosion mechanisms in wet sour gas systems containing significant CO2[J].Corrosion/1996.Houston:NAcE,1996,Paper No.26.
[31] Hoffmeister H.Modeling the effect of chloride content on H2S corrosion by coupling of phase and polarization behavior[J].Corrosion/2007.Houston:NACE,2007,Paper No.07501.
[32] Vitale D D.Effect of hydrogen sulfide partial pressure,pH and chloride content on the SSC resistance of marteasitic stainless steels and rnartensitic precipitation hardening stainless steels[J].Corrosion/1999.Houston,1999,Paper No.584.
[33] Salih S A,Mazhar A A,Mahanny H.The effect of sour gases and some anions on the corrosion behavior of carbon steel[J].Ponugaliae Electrochimica Acta,2004,22(3):205.
[34] Pots B F M,John R C,Rippon I J,et al.Improvements on de waard-milliams corrosion prediction and applications to corrosion management[J].Corrosion/2002.Houston:NACE,2002,Paper No.02235.
[35] Omar I H,Gunaltun Y M,Kvarekval J,et al.H2S corrosion of carbon steel under simulated kashagan field conditions[J].Corrosion/2005.Houston:NACE,2005,Paper No.05300.
[36] NACE MR0175-2001,Sulfide stress cracking resistant metallic materials for oilfield equipment[S].
[37] NACE TM0177-2005,Laboratory testing of metals for resistanee to sulphide stress cracking and stress corrosion cracking in H2S environments[S].
[38] NACE TM0284-2003,Evaluation of pipeline and pressure vessel steels for resistance to hydrogen induced cracking[S].
[39] EFC Publications No.16,Guidelines on materials requirements for carton and low alloy steels for H2S-containing environments in oil and gas production[S].
[40] EFC Publications No.17,Corrosion resistant alloys for oil and gas production:Guidelines on general requirements and test methods for H2S service[S].
[41] ISO 15156-1:2001,Petroleum and natural gas industries-Materials for use in H2S-containing environments in oil and gas production-Partl:General principles for selection of cracking-resistsnt materials[S].
[42] ISO 15156-2:2003,Petroleum and natural gas industries-Materials for use in H2S-containing environments in oil and gas production-Part2:Cracking-resistant carbon and low alloy steels,and the use of irons[S].
[43] ISO 15156-3:2003,Petroleum and natural gas industries-Materials for use in H2S-containing environments in oil and gas production-Part3:Cracking-resistant CRAs (corrosion-resistant alloys) and other alloys[S].
[44] 张忠铧,郭金宝,蔡海燕,等.经济型抗CO2、H2S腐蚀油套管的开发[J].试验与研究,2004,33(5):18.
[45] 植田吕克,Ueda M.合金元素和显微结构对CO2/H2S环境中腐蚀产物稳定性的影响[J].石油与天然气化工,2005,34(1):43.
[46] Klein L J,Thompson R M,Meore D E.9Cr-IMo and 13Cr tubules for sour service[J].Corrosion/1990.Houston:NACE,1990,Paper No.52.
[47] Kermanin B J,Martin J,Esaklul K,et al.Materials design strategy:Effects of H2S/CO2 corrosion on materials selection[J].Corrosion/2006.Houston:NACE,2006,Paper No.06121.
[48] Kimura M,Sakata K,Shimamoto K,et al.SCC performance of martensitic stainless steel OCTG in packer fluid[J].Corrosion/2006.Houston:NACE,2006,Paper No.06137.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%