分析了以普碳钢成分生产的超细晶粒钢的显微组织.结果表明:工业生产的超细晶粒钢的显微组织由铁素体和珠光体组成,铁素体的晶粒尺寸为4~5 μm,组织中珠光体所占体积分数较低.珠光体中渗碳体以短棒状或颗粒状存在,细小的铁素体晶粒使晶粒内的位错塞积密度减少,有利于提高钢的强度和韧性.
参考文献
[1] | Montemarano T W .High Strength Low Alloy Steels in Naval Construction[J].Journal of Ship Production,1986,2(03):145-162. |
[2] | Yada H;Matsumura Y.A New Thermomechanical Heat Treatment for Grain Refining in Low Carbon Steels[A].ISIJ,Tokyo,1988:200. |
[3] | P.D.Hodgson;M.R.Hickson;R.K.Gibbs .ULTRAFINE FERRITE IN LOW CARBON STEEL[J].Scripta materialia,1999(10):1179-1184. |
[4] | Beynon J H;Gloss R;Hodgson P D.The Production of Ultrafine Equiaxed Ferrite in A Low Carbon Steels Microalloyed Steel by Thermomechanical[A].,1992:37-42. |
[5] | Hurley P J;Hodgson P D.Analysis and Characterisation of Ultra-fine Ferrite Producced during A New Steel Ship Rolling Process[A].,1999:433-438. |
[6] | P.D.Hodgson;M.R.Hickson .The production and mechanical properties of ultrafine ferrite[J].Materials Science Forum,1998(0):63-72. |
[7] | Choo Wung-yong.Present developing status of high performance steel in korea(HIPERS-21 Project)[A].北京,2001:16-26. |
[8] | Inoue T;Torizuka S;Nagai K.Effect of Plastic Strain on Grain Size of Ferrite Transformed from Deformed Austenite in Si-Mn Steel[A].物质材料研究机构,平成13年度:45-53. |
[9] | 雍歧龙;马鸣图;吴宝榕.微合金钢-物理与力学冶金[M].北京:机械工业出版社,1989:57-59,104. |