高级检索

综述了近10年来国内外对高速干滑动摩擦磨损行为的研究成果,总结了不同条件下材料的摩擦磨损机理,对影响高速摩擦磨损性能的因素进行了分析,并提出了高速摩擦学研究中存在的问题及研究方向.

参考文献

[1] Jun Jiang;Heinz Ulbrich .Derivation of coefficient of friction at high sliding speeds from energy conservation over the frictional interface[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2001(1):66-75.
[2] Irfan MA.;Prakash V. .Time resolved friction during dry sliding of metal on metal[J].International Journal of Solids and Structures,2000(20):2859-2882.
[3] BRYANT M D;WANG J P;LIN J W .Thermal mounding in high speed dry slider:experiment,theory and comparison[J].Wear,1995,181-183:668-677.
[4] Rajagopalan S.;Prakash V.;Irfan M.A. .Novel experimental techniques for investigating time resolved high speed friction[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,1999(2):1222-1237.
[5] D. Severin;S. Dorsch .Friction mechanism in industrial brakes[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2001(9):771-779.
[6] M. Reyes;A. Neville .Degradation mechanisms of Co-based alloy and WC metal-matrix composites for drilling tools offshore[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2003(7/12):1143-1156.
[7] Ranga Komanduri;Zhen Bing Hou .Thermal analysis of dry sleeve bearings - a comparison between analytical, Numerical (finite element) and experimental results[J].Tribology International,2001(3):145-160.
[8] Margam Chandrasekaran;Andrew William Batchelor;Nee Lam Loh .Frictional seizure of aluminium observed by X-ray imaging[J].Tribology International,2002(5):297-308.
[9] H. So;D. S. Yu;C. Y. Chuang .Formation and wear mechanism of tribo-oxides and the regime of oxidational wear of steel[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2002(9/10):1004-1015.
[10] SO H .The mechanism of oxidational wear[J].Wear,1995,184:161-167.
[11] S. C. Lim .The relevance of wear-mechanism maps to mild-oxidational wear[J].Tribology International,2002(11):717-723.
[12] WOYDT M;SKOPP A;D(O)RFEL I;WITKE K .Wear engineering oxides and anti-wear oxides[J].Wear,1998,218:84-95.
[13] LIM S C;ASHBY M F .Wear-mechanism maps[J].Acta Metalluraica,1987,35:1-24.
[14] S. C. Lim .Recent developments in wear-mechanism maps[J].Tribology International,1998(1/3):87-97.
[15] 张永振,邱明,上官宝,铁喜顺,马东辉.高速干摩擦条件下铝基复合材料的摩擦磨损行为研究[J].摩擦学学报,2005(04):343-347.
[16] Tiejun Ma;Hideki Yamaura;Donald A. Koss .Dry sliding wear behavior of cast SiC-reinforced Al MMCs[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2003(1/2):116-125.
[17] Degnan CC.;Wood JV.;Shipway PH. .Elevated temperature sliding wear behaviour of TiC-reinforced steel matrix composites[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2001(2):1444-1451.
[18] Wilson S;Alpas AT .Effect of temperature and sliding velocity on TiN coating wear[J].Surface & Coatings Technology,1997(1/3):53-59.
[19] MURATOGLU M;AKSOY M .The effects of temperature on wear behaviours of Al-Cu alloy and Al-Cu/SiC composite[J].Materials Science and Engineering A-structural Materials Properties Microstructure and Processing,2000,282:91-99.
[20] REDDY A S;BAI B N P;MURTHY K S S et al.Mechanism of seizure of aluminium-silicon alloys dry sliding against steel[J].Wear,1995,181-183:658-667.
[21] Chong Ching Chang;Jen Fin Lin;Chung Yi Chen;Chi-Fong Ai .The effect of under-layers and pre-test temperature on the tribological characteristics of TiN films rubbing against steel[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2004(3/4):252-267.
[22] K. M. Shorowordi;A. S. M. A. Haseeb;J. R. Celis .Velocity effects on the wear, friction and tribochemistry of aluminum MMC sliding against phenolic brake pad[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2004(11/12):1176-1181.
[23] S. K. Biswas .Some mechanisms of tribofilm formation in metal/metal and ceramic/metal sliding interactions[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2000(1/2):178-189.
[24] DEGNAN C C;SHIPWAY P H .A comparison of the reciprocating sliding wear behaviour of steel based metal matrix composites processed from serf-propagating high-temperature synthesised Fe -TiC and Fe -TiB2masteralloys[J].Wear,2002,252:832-841.
[25] AKSOY M;KARAMIS M B;EVIN E .An evaluation of the wear behaviour of a dual-phase low-carbon steel[J].Wear,1996,193:248-252.
[26] SINGH J;ALPAS A T .Dry sliding wear mechanisms in a Ti50Ni47Fe3 intermetallic alloy[J].Wear,1995,181-183:302-311.
[27] D. Y. Li;Rong Liu .The mechanism responsible for high wear resistance of pseudo-elastic TiNi alloy--a novel tribo-material[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,1999(2):777-783.
[28] MOLINARI A;STRAFFELINI G;TESI B et al.Dry sliding wear of Ti6A14V alloy as influenced by the counterface and sliding conditions[J].Wear,1997,208:105-112.
[29] CHEN Z;LIU P;VERHOEVEN J D et al.Tribologicai behavior of Cu-20% Nb and Cu-15% Cr in situ composites under dry sliding conditions[J].Wear,1996,199:74-81.
[30] MOLINARI A;STRAFFELINI G;TESI B et al.Effects of load and sliding speed on the tribological behaviour of Ti-6Al-4V plasma nitrided at different temperatures[J].Wear,1997,203-204:447-454.
[31] 居毅.碳钢表面碳-氮共渗层在高速干摩擦条件下的摩擦学性能研究[J].摩擦学学报,2002(01):71-74.
[32] J. E. Fernandez;Yinglong Wang;R. Tucho;M. A. Martin-Luengo;R. Gancedo;A. Rincon .Friction and wear behaviour of plasma-sprayed Cr_2O_3 coatings against steel in a wide range of sliding velocities and normal loads[J].Tribology International,1996(4):333-343.
[33] Yongqing Fu;Nee Lam Loh;Jun Wei;Bibo Yan;Peter Hing .Friction and wear behaviour of carbon nitride films deposited on plasma nitrided Ti-6Al-4V[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2000(1):12-19.
[34] Thananan Akhadejdarmrong;Tatsuhiko Aizawa;Michiko Yoshitake;Atsushi Mitsuo;Takahisa Yamamoto;Yuichi Ikuhara .Self-lubrication mechanism of chlorine implanted TiN coatings[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2003(7/8):668-679.
[35] S. Wilson;H. M. Hawthorne;Q. Yang;T. Troczynski .Sliding and abrasive wear of composite sol-gel alumina coated Al alloys[J].Surface & Coatings Technology,2000(0):389-396.
[36] M. Scherge;D. Shakhvorostov;K. Pohlmann .Fundamental wear mechanism of metals[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2003(1/6):395-400.
[37] Kia-Moh Teo;Khalid Lafdi .Effect of Thermal Property Variation on Surface Grooving[J].Journal of Tribology,2002(2):274-280.