浇注过程中水口(定径水口、浸入式水口)堵塞是影响连铸机产量和铸坯质量的一个障碍,长期以来人们对于浇注过程中中间包水口堵塞现象做过许多研究.结合相关工作和有关文献,对浇注铝镇静钢(Al-K)和硅镇静钢(Si-K)水口堵塞现象、水口堵塞的机理以及防止水口堵塞的技术措施进行了评述.
参考文献
[1] | 张立峰;蔡开科.BOF-RH-CC生产纯净钢研究报告[J].北京科技大学学报,1998(05):73. |
[2] | F. Fuhr;C. Cicutti;G. Walter .Relationship Between Nozzle Deposits and Inclusion Composition in the Continuous Casting of Steels[J].Iron & Steelmaker,2003(12):53-58. |
[3] | 张立峰;蔡开科.BOF-RH-CC生产纯净钢研究报告[J].北京科技大学学报,1998(05):58. |
[4] | 魏军 .BOF-LF-CSP流程低碳铝镇静钢非金属夹杂物行为研究[D].北京科技大学,2005. |
[5] | J.D.Murray.Special steel production by high integity billet casting[A].,1985 |
[6] | Gregoryl.Dressed.High Carbon Silicon -killed Steel Nozzle Clogging[J].I & SM,2003:26. |
[7] | Scott R.Story;Gerry E.Goldsmith;Richard J.Fruehan.A Study of Casting Issue Using Rapid Inclusion Identification and Analysis[J].Iron and Steel Technology,2006:53. |
[8] | Luis Trueba Jr;Kent D.Peasis;Jeffreg D.Smith .Effect of Nozzle Base Material on the Rate of Clogging During the Continuous Casting of Al-K Steel[J].Steel Research International,2006,77(01):38. |
[9] | K Ahlbory,Seven.Ways to Shut Down The Caster[A].:861. |
[10] | 国际钢铁协会;中国金属学会.洁净钢-洁净钢生产工艺技术[M].北京:冶金工业出版社,2006 |
[11] | M.Burty;L.Peeters;E.Peerin.Some keys to reach long-sequence casting[A].:462. |
[12] | P.Valentin;C.Bruch;H,Kochner;T.Lamp.铝脱氧钢夹杂物工程-获得优良可浇性和高洁净度[A].,2004:109. |
[13] | P.Guillo;J.Simoes.钢水夹杂物组成对钢水可浇性影响[A].,2004:39,91. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%