研究了镍基单晶高温合金DD3(001),(011),(111)取向光滑圆拉伸试样在760℃,850℃,950℃典型应力条件下的拉伸蠕变特征.试验发现,在较高蠕变应力水平时,DD3单晶合金具有明显且复杂的拉伸蠕变各向异性,且蠕变变形率及其对应力增加的敏感性的强弱顺序会随温度变化而发生变化.这归因于该合金的成分特征、蠕变应力、晶体取向决定的蠕变主滑移系类型(八面体、立方及二者混合)及位错移动动力学特点的不同.
参考文献
[1] | SHAH D M;CETEL A.Creep anisotropy in nickel base γ,γ′ and γ/γ′ superalloy[A].,1996:273. |
[2] | SASS V;SIEBOEGE D R;DNOCBLOCH C.Anisotropy creep behavior of a nickel-based superalloy compared with nickel solid solution and single crystal[A].,1997:687. |
[3] | HENDERSON P J;LINDBLOM J;LINDE L.Creep of single crystal Ni-base superalloyin thick and thin-section forms[A].,1997:697. |
[4] | MACKAY R A;MAYER R D .The influence of orientation on the stress rupture properties of nickel-based single crystal superalloy[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1982,13:1747. |
[5] | SASS V;GLATIEL U;FELLER-KNEIPMEIER M.Creep anisotropy in the monocrystal nickel-base superalloy[A].,1996:283. |
[6] | HOPGOODAND A A;MARTIN J W .The creep behavior of nickel-base single crystal superalloy[J].Materials Science and Engineering R:Reports,1986,82:27. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%