文章主要综述了AB2型Laves相贮氢合金的种类及性能特点以及合金化及制备工艺对合金电化学性能的影响.介绍了AB2型Laves相贮氢合金研究的国内外动态及目前达到的水平,对AB2型Laves相贮氢合金未来的研究重点及发展方向提出了看法.

参考文献

[1] Vucht H N;Kuijpers F A;Bruning H C A M.[J].Philips Research Reports:133.
[2] 郑青榕;顾安忠.[J].新能源(12):120.
[3] 鲍德佑.[J].太阳能学报,1995(01):114.
[4] Bogdanovic B;Hartwig T H;Splieth off B.[J].International Journal of Hydrogen Energy,1993(07):575.
[5] Zuttel A;Meli F;Schlapbach L.[J].Journal of Alloys and Compounds,1994:31.
[6] Villars P;Calvert L D.Person's Handbook Crystallographic Data For Intermetallic Phases[M].ASM International,Materials Park,OH,1993:4406.
[7] Villars P;Calvert L D.Person's Handbook Crystallographic Data for Intermetallic Phases[M].ASM International,Materials Park,OH,1993:5354.
[8] Pebler A;Gulbransen E A.[J].Electrochemical Technology:211.
[9] Pebler A;Gulbransen E A.[J].Transactions of the Metallurgical Society of AIME:1593.
[10] Gamo T;Moriwaki Y et al.[J].International Journal of Hydrogen Energy,1985,10:39.
[11] 山下敏夫;蒲生孝治.[J].日本金属学会志(日本):148.
[12] 张文魁,马淳安,黄辉,杨晓光,涂江平,雷永泉.Zr-Mn-V-Ni储氢电极合金中的Zr-Ni相形成及其晶体结构研究[J].稀有金属材料与工程,2001(03):194-197.
[13] Joubert J M;Latrochen M.[J].Journal of Alloys and Compounds,1996:219.
[14] Liu F J;Suda S;Sandrock G.[J].Journal of Alloys and Compounds,1996:232.
[15] Moriwaki Y;Gamo T.[J].Journal of the Less-Common Metals:1028.
[16] Moriwaki Y;Gamo T.[J].Journal of the Less-Common Metals:1211.
[17] Yu J Y;Lei Y Q;Chen C P.[J].Journal of Alloys and Compounds,1995:578.
[18] 杨晓光;张志鸿;等;中国材料研究学会编.94秋季中国材料研讨会会议论文集[C].北京:化学工业出版社,1995:403.
[19] Yang X G;Lei Y Q.[J].Journal of Alloys and Compounds,1996:151.
[20] 李平 .快淬低钴AB<,5>型和快淬钛基AB<,2>型储氢合金的研究[D].钢铁研究总院,2002.
[21] Wakao S;Sawa H J.[J].Journal of the Less-Common Metals:1219-1226.
[22] Sawa H;Wakao S.[J].Materials Transactions:487.
[23] Chen J.;Dou SX.;Liu HK.;Bradhurst DH. .Surface and electrode properties of Zr(V0.25Ni0.75), alloy treated with ultrasound-solution[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,1998(1/2):281-285.
[24] Kim Dong-Myung;Lee Sang-Min.[J].Journal of Alloys and Compounds,1998:241.
[25] Hagstrom MT.;Lund PD.;Vanhanen JP. .AB(2) metal hydrides for high-pressure and narrow temperature interval applications[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,1998(1/2):288-293.
[26] Moriwaki Y;Camo T;Iwaki T.[J].Journal of the Less-Common Metals
[27] Liu Binhong;Kim D M;Lee Kiyoung.[J].Journal of Alloys and Compounds,1996:214.
[28] Hagstrom MT.;Lund PD.;Vanhanen JP. .AB(2) metal hydrides for high-pressure and narrow temperature interval applications[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,1998(1/2):288-293.
[29] 李平,王新林,吴建民,祁焱,李蓉.铸态和快淬Ti基贮氢合金的放电容量与显微结构[J].中国有色金属学报,2002(05):902-906.
[30] Gao Xueping;Song Deying et al.Electrochemical and surface properties of the Zr(V0.2Mn0.2Ni0.6)2.4 alloy electrode[J].JAIloys Comp,1995,229:268.
[31] Yan deyi;Gary Sandrock;Seijirau Suda .Activation of Zr0.5 Ti0.5V0.75Ni1.25 alloy electrodes by hot alkaline solutions[J].Journal of Alloys and Compounds,1994,216:237.
[32] Chang Bo Jung;Jee Ko Kin;Kyung Sub Lee.[J].Journal of Alloys and Compounds,1998:265.
[33] Sun Dalin;Joubert J M et al.Metallurgical state of lanthanum and its effects on the activation behaviour of Zr(Cr0.4Ni0.6)2 hydride formation[J].Journal of Alloys and Compounds,1996,231(02):193-197.
[34] Chen J;Dou S X;Liu H K.[J].Journal of Alloys and Compounds,1997:146.
[35] Ovshinky J R.[J].SCIENCE,1993:176.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%