采用柠檬酸络合无焰燃烧法制备锂离子电池正极材料尖晶石型LiMn2O4,颗粒大小只有10-100nm,晶型完整,电化学性能与国内外商品化的同种材料相当.直流电阻实验显示该材料在低于室温处存在一个相变.采用柠檬酸络合无焰燃烧法可以简化柠檬酸络合反应法的制备工艺,降低其成本.
参考文献
[1] | Koksbang R.;Shi H.;Saidi MY.;Barker J. .CATHODE MATERIALS FOR LITHIUM ROCKING CHAIR BATTERIES [Review][J].Solid state ionics,1996(1/2):1-21. |
[2] | Thackeray M M;Johnson P J;Picciotto de L A .[J].Materials Research Bulletin,1984,19:179-187. |
[3] | Manev V;banov B;A momchilov et al.[J].Journal of Power Sources,1995,57:9. |
[4] | Yang Wensheng;Qui Weihua;Lu Shigang;Yang Leiling;Lui Qinggguo .Citric acid method to prepare LiMn_2O_4 for lithium-ion batteries[J].Solid state ionics,1999(1/4):79-84. |
[5] | Yoshio M;Noguchi H;Miyashita T et al.Sources[J].Journal of Power Sources,1995,54:483. |
[6] | Choy J H;Kim D H;Kwon C W et al.[J].Journal of Power Sources,1999,77:1-11. |
[7] | 李群,卢世刚,邱向东.阴极材料正尖晶石LiMn204制备方法研究现状[J].电源技术,1999(05):289. |
[8] | Oikawa;Kamiyama T;Izumi F et al.[J].Solid State Ionics,1998,109:35. |
[9] | Gummov R J;Thackeray M M .Soc[J].Journal of the Electrochemical Society,1994,141(05):1178. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%