采用传统的氧化物固溶工艺制备了(Na0.51K0.44Li0.05)Nb092Ta0.08O3和助烧剂Na5.4Cu13Sb10O29.对(Na0.51K044Li0.05)Nb0.92Ta0.08O3添加助烧剂Na5.4Cu1.3Sb10O29的研究表明,助烧剂能大幅度提高(Na0.51K0.44Li0.05)Nb0.92Ta0.08O3的压电和机电耦合性能.质量百分比为4%Na5.4Cu1.3Sb10O29掺杂的(Na051K0.44Li0.05)Nb092Ta0.08O3具有高的压电应变常数(d33=266pC/N),高的机电耦合系数kt(46.7%)、k33(63.7%),较低的损耗(tanδ=1.8%),和高的居里温度(391℃).这些参数表明,Na5.4Cu1.3Sb10O29掺杂的(Na0.51K0.44Li0.05)Nb0.92Ta0.08O3是替代锆钛酸铅且具有很好的应用前景的无铅压电陶瓷.
参考文献
[1] | Saito Y;Takao H;Tani T et al.Lead-free piezoceramics[J].Nature(London),2004,42:84-87. |
[2] | Masato MATSUBARA;Toshiaki YAMAGUCHI;Koichi KIKUTA;Shin-ichi HIRANO .Sintering and Piezoelectric Properties of Potassium Sodium Niobate Ceramics with Newly Developed Sintering Aid[J].Japanese journal of applied physics,2005(1A):258-263. |
[3] | Matsubara M;Kikuta K;Hirano S .Piezolectric Properties of (Na0.5K0.5) (Nb1-xTax) O3-K5.4Cu1.3Ta10O24 Ceramics[J].Journal of Applied Physics,2005,44:258-263. |
[4] | Yiping Guo;Ken-ichi Kakimoto;Hitoshi Ohsato .Phase transitional behavior and piezoelectric properties of (Na_(0.5)K_(0.5))NbO_(3)-LiNbO_(3) ceramics[J].Applied physics letters,2004(18):4121-4123. |
[5] | 张沛霖;钟维烈.压电材料与器件物理[M].济南:山东科学技术出版社,1997:176-177. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%