以Al2O3为骨料,添加一定数量的烧结促进剂,通过挤出成型,在介于1100~1400℃之间的温度下烧成.制备出管式多孔陶瓷支撑体.考察了保温时间对多孔支撑体性能的影响.得到具有较高孔隙率、较好渗透性能、较高机械强度以及良好耐腐蚀性能的管式多孔氧化铝支撑体.
参考文献
[1] | Bhave R R.Inorganic membranes synthesis, characteristics and applications[M].New York: Van Nostrand Reinhold,1991 |
[2] | Hsieh H P.Inorganic membrane for separation and reaction[M].Amsterdam: Elesevier Science B V,1996 |
[3] | 王焕庭;刘杏芹;周勇 等.多孔陶瓷支撑体膜材料的制备与性能表征[J].膜科学与技术,1997,17(01):47-52. |
[4] | 黄肖容;黄仲涛 .熔模离心法制备高纯氧化铝基质膜管[J].膜科学与技术,1996,16(02):31-37. |
[5] | 吴皆正;易石阳;欧阳琨 .可控微米级多孔陶瓷的研制[J].硅酸盐通报,1993,3:4-9. |
[6] | Saracco G;Versteeg G F;Swaaij W P M van .Current hurdles to the success of high temperature membrane reactors[J].Journal of Membrane Science,1994,95(02):105-123. |
[7] | Biesheuvel P. Maarten;Verweij Henk .Design of ceramic membrane supports: Permeability, tensile strength and stress[J].Journal of Membrane Science,1999(1):141-152. |
[8] | 黄培,邢卫红,徐南平,时钧.气体泡压法测定无机微滤膜孔径分布研究[J].水处理技术,1996(02):80. |
[9] | Coble R R .Initial sintering of alumina and hematite[J].Journal of the American Ceramic Society,1958,41(02):55-62. |
[10] | Kingery W D;Bowen H K;Uhlmann D R.Introduction to ceramics[M].New York:John Wiley & Sons,1976:131-139,448-490. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%