对粉末冶金法制备的纯Mo及Mo-43wt%Re合金不同状态下的力学性能和显微组织变化研究,结果表明:Mo-43wt%Re合金较纯Mo加工硬化显著,冷轧态纯Mo硬度仅为340HV,而Mo-43wt%Re合金的硬度达420HV.同时,Mo-43wt%Re合金抗高温软化性能较纯Mo得到显著提高,纯Mo的再结晶开始温度为900℃左右,Mo-43wt%Re合金在1350~1400 ℃开始再结晶,且再结晶晶粒细小,此时合金硬度较低,冷加工性能较好,可进行的最大变形量达50%.冷轧态Mo-43wt%Re合金出现大量位错胞组织,随着退火温度的升高,位错密度不断降低,且在不同温度下分别出现了均匀的螺位错网络和波浪形位错等组织.

参考文献

[1] Geach G A;Hughes J E.The alloys of rhenium with molybdenum or with tungsten and having good high temperature properties[A].London:Pergamon,1956
[2] Stephens J R;Witzke W R .Alloy softening in group via metals alloyed with rhenium[J].Journal of the Less Common Metals,1971,23:325.
[3] Gypen L A;Deruyttere A .Multi-component intrinsic solid solution softening and hardening[J].Journal of the Less Common Metals,1977,56:91.
[4] Todd L;Carlen J C;Martin B.Investigation of mechanical properties and microstructure of various molybdenum-rhenium alloys[A].,1999:685.
[5] Mannheim R L;Garin J L .Strain hardening of rhenium and two typical molybdenum-rhenium alloys manufactured by powder sintering[J].Zeitschrift fur Metallkunde,2000,91:848.
[6] Wright N .A study of various contributions to substructural strengthening in Mo-33Re rolled to large strains[J].Materials Science and Engineering A,1988,104:85.
[7] Mahajan S .Observations on the interaction of twins with grain boundaries in Mo-35at% Re alloy[J].Acta Metallurgy,1973,21:255.
[8] Davidson D L;Brotzen F R .Plastic deformation of molybdenum-rhenium alloy crystals[J].Acta Metallurgica,1970,18:463.
[9] S. R. Agnew;T. Leonhardt .The Low-Temperature Mechanical Behavior of Molybdenum-Rhenium[J].JOM,2003(10):25-29.
[10] Carlen J C;Bryskin B D .Concerning sigma-phase in molybdenum-rhenium alloys[J].Journal of Materials Engineering and Performance,1994,3(02):282.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%