以MoS2、TiC、Ni粉为原料,在20钢基材表面利用激光熔覆技术制备了减摩耐磨复合涂层.采用SEM和XRD对复合涂层的组织和相组成进行了研究,结果表明复合涂层主要由部分未熔的TiC颗粒、Mo2C、γ镍基固溶体和多种两元、三元硫化物TiS、NiS、Ni3Ti4S8等组成.用FALEX-6摩擦磨损实验机对MoS2/TiC/Ni复合涂层、MoS2/Ni激光熔覆层以及45钢的耐磨性能进行了对比,并对三种试样表面的磨损形貌进行了SEM观察.实验表明:MoS2/Ni激光熔覆层具有最低的摩擦系数,但磨损失重最大;MoS2/TiC/Ni复合涂层在载荷17.8N、转速200r/min条件下,磨损40分钟,其磨损失重仅为45钢的1/6.

参考文献

[1] L C Lim et al.Microstructures of lasor-clad nickel-based hardfacing alloys[J].Surface and Coatings Techonology,1998,106:183-192.
[2] A Hidouci et al.Microstructural and mechanical characteristics of laser coatings[J].Surface and Coatings Techonology,2000,123:17-23.
[3] B.J. Kooi;Y.T. Pei;J.Th.M. De Hosson .The evolution of microstructure in a laser clad TiB-Ti composite coating[J].Acta materialia,2003(3):831-845.
[4] Roberts Wyn .New frontiers for space tribology[J].Tribology International,1990,23(02):149-155.
[5] H E Sliney .Solid lubricant materials for high temperatures review[J].Tribology International,1982,10:303-314.
[6] G HLiu et al.Improvement in tribolngical properties of chromiumoxide coating at high temperature by solid lubricants[J].Wear,1993,160:181-189.
[7] 曾德麟.粉末冶金材料[M].北京:冶金工业出版社,1989:174.
[8] WangZK;ZhengQG;TaoZY .[J].Acta Metallurgica Sinica,1999,35(10):1027-1030.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%