将预活化的沥青基炭球在不同金属盐的水溶液中浸渍,使之负载有金属,然后进行活化处理.结果发现:活化过程中氢气的存在可以提高铁、钴、镍催化活化反应速度,但对钇催化的活化反应速度却有抑制作用.在氢气存在条件下制得的沥青基球状活性炭的中孔主要分布在30~50nm处,而在氮气气氛中制得的中孔主要分布却在2.0nm处.
参考文献
[1] | E E Alexandroff .[J].NBC Defense and Technology International,1986,I(02):44. |
[2] | Europan Patent 9688566[M]. |
[3] | 乔文明,王克温,凌立成,刘朗,周承泽,王瑾,郑斌.不熔化沥青球在低速流化床中炭化和活化的初步研究[J].燃料化学学报,1996(04):375-378. |
[4] | 刘植昌;凌立成;乔文明;刘朗 .[J].炭素技术,1996,4:22. |
[5] | 宋燕;凌立成;乔文明.[A].,1997:239. |
[6] | Rodrigez-Reinoso,F;Almela-Alarcon,M;Linares-Solano,A;et a l.Extended Abstracts,17th Biennial Conference on Carbon[M].,1985:273. |
[7] | Marsh,H;and Rand,B .[J].Carbon,1971,9:63. |
[8] | Tamai,H;Kojima,S;Ikeuchi,M et al.[J].TANSO,1996,175:243. |
[9] | Marsh,H;Diez,M A;Kuo,J;J.Lahaye and P.Ehrburgor.in Fundamental issues in control of carbon gasification reactivity[M].Kluwer Academic Pu blishers,1991:205. |
[10] | Tomita,A;Higashiyama,K;Tamai,Y .[J].Fuel,1981,60:103. |
[11] | McKee,D W .[J].Carbon,1974,12:453. |
[12] | McKee,D W;P L Walker,Jr;P A Th rower.inChemistry and Physics of Carbon[M].Marcel Dekker New York,1981:16:1. |
[13] | Matsumoto,S;and Walker,P L,Jr .[J].Carbon,1986,24:277. |
[14] | Walker,P L,Jr;Matsumoto,S et al.[J].Fuel,1983,62:140. |
[15] | Walker,P L,Jr;Rusinko,F,Jr;et al;D.D.Eley , P.W.Selwook and P.B.Weisz.in Advances in Catalysis[M].Academic Press New York,1959:133. |
[16] | 王克温;乔文明;刘植昌 .[J].炭素技术,1996,2:5. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%