本文研究了退火态6. 5%Si-Fe热轧合金在不同温度下拉伸时的力学性能,并观察了拉伸断口形貌及退火态6.5%Si-Fe热轧合金的金相组织.结果表明,经750℃保温140min后,6.5%Si-Fe热轧合金的层状组织消除;其断裂模式随拉伸温度的升高迅速由解理断裂向韧性断裂转变;在200℃拉伸时,为纯解理断口,此时该合金即具有高达26%的延伸率;但是在200℃-400℃温区,延伸率未随温度的升高而显著增大,其断口形貌为解理+韧窝的混合断口;在500℃拉伸时,为纯韧窝断口,其延伸率可达43%.

参考文献

[1] W E Ruder .New Magnetic Materials[J].Proc Inst Radio Engrs,1942,30:437-440.
[2] K Narita;M.Enokizono .Effect of Nickel and Manganese Addition on Ductility and Magnetic Properties of 6.5% Silicon-Iron Alloy[J].IEEE Transactions on Magnetics,1978,MAG14:258-262.
[3] K I Arai;H Tsutsumitake;K Ohmori .Grain Growth and Texture Formation by Annealing of Rapidly Quenched High Silicon-Iron Alloy[J].Transactions of the Japan Institute of Metals,1984,25:855-862.
[4] 刘海明;彭长平;李玉国 .Fe|6.5%Si快速凝固极薄带[J].钢铁,1993,28(07):55-59.
[5] Y Takada;M Abe;S.Masuda;J.Inagaki .Commercial Scale Production of Fe-6.5wt.%Si Sheet and its Magnetic Properties[J].Journal of Applied Physics,1988,64:5367-5369.
[6] 何忠治.电工钢[M].北京:冶金工业出版社,1996:975-1006.
[7] 谢燮揆 .高硅电工钢[J].中小型电机,1994,21(03):60-61.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%