以Cr35 Ni45 Nb合金钢为对象进行一系列高温蠕变持久试验,并采用SEM、EDS等对试样外表面、横截面及断口进行了观察分析.结果表明,蠕变过程中Cr35Ni45Nb的氧化腐蚀对持久寿命的影响较大,它主要取决于表面氧化膜破裂-自修复和内氧化两种行为的耦合过程;当氧化膜失去保护作用后,严重的内氧化过程将逐渐向心部扩展,使得晶界强度急剧弱化,材料的有效承载面积减小,从而加速材料的蠕变进程.另外,高温应力环境下Cr35Ni45Nb钢中会同时发生一次碳化物聚合粗化、析出相粒子数目减少、内氧化等化学损伤,以及蠕变空洞的形核长大甚至裂纹的形成等机械应力损伤,这两种损伤相互促进,导致炉管材料组织及力学性能弱化,持久寿命降低,Larson-Miller参数法外推的持久寿命发生一定程度的偏离.
参考文献
[1] | Khodamorad S H,Haghshenas Fatmehsari D,Rezaie H,et al .Analysis of ethylene cracking furnace tubes[J].Engineering Failure Analysis,2012,21 |
[2] | Mitchell D,Young D J,Kleemann W .Caburisation of heat-resistant steels[J].Materials and Corrosion,1998,49(4):231-236.,1998. |
[3] | Kaya A A,Krauklis P,Young D J .Microstructure of HK40 alloy after high temperature service in oxidizing/carburizing environment[J].Materials Characterization,2002,49(1):11-34.,2002. |
[4] | Zhu Z,Cheng C,Zhao J,et al .High temperature corrosion and microstructure deterioration of KHR35H radiant tubes in continuous annealing furnace[J].Engineering Failure Analysis,2012,21 |
[5] | Petkovic-Luton R,Ramanarayanan T A .Mixed-oxidant attack of high-temperature alloys in carbon-and oxygen-containing environments[J].Oxidation of Metals,1990,34:381-400.,1990. |
[6] | 李铁藩.金属高温氧化和热腐蚀[M].北京:化学工业出版社,2003.,2003. |
[7] | Tempest P A,Wild R K .Oxidation pretreatment to reduce corrosion of 20% Cr-25% Ni-Nb stainless steel[J].Oxidation of Metals,1988,30:209-254.,1988. |
[8] | 周长海,马海涛,王来.外加应力下合金高温氧化膜的生长及其失效愈合研究现状[J].腐蚀科学与防护技术,2010(06):558-562. |
[9] | 钱余海,李美栓,张亚明.力学载荷作用下合金的高温氧化行为研究状况[J].腐蚀科学与防护技术,2001(06):342-346. |
[10] | Young D J.High temperature oxidation and corrosion of metals[M].Access Online via Elsevier,2008.,2008. |
[11] | Ling S,Ramanarayanan T A,Petkovic-Luton R .Computational modeling of mixed oxidation-carburization processes:Part 1[J].Oxidation of Metals,1993,40:179-196.,1993. |
[12] | 李美栓.金属的高温腐蚀[M].北京:冶金工业出版社,2001.,2001. |
[13] | 张俊善.材料的高温变形与断裂[M].北京:科学出版社,2007.,2007. |
[14] | Robertson J,Manning M I .Limits to adherence of oxide scales[J].Materials Science and Technology,1990,6(1):81-92.,1990. |
[15] | 钱余海,李美栓,张亚明.氧化膜开裂和剥落行为[J].腐蚀科学与防护技术,2003(02):90-93,100. |
[16] | 靳惠明,Felix A,Aroyave M .离子注钇对镍900℃高温氧化行为及氧化膜性能的影响研究[J].物理学报,2006,55(11):6157-6162.JIN Hui-ming,Felix A,Aroyave M.Influence of yttrium ion-implantation on oxidation behavior of nickel and property of oxide scale at 900 ℃[J].Acta Physics Sinica,2006,55(11):6157-6162.,2006. |
[17] | 辛丽,李铁藩 .离子注入Y+对Ni30Cr定向凝固合金氧化膜界面缺陷与剥落机制的影响[J].金属学报,1997,33(8):851-862.XIN Li,LI Tie-fan.Influence of Y+-implanation on interfacial defects and spalling mechanism of Cr2O3 scale formed on Ni30Cr directional solidification alloy[J].Acta Metallurgica Sinica,1997,33 (8):851-862.,1997. |
[18] | Riedel H.Fracture at High Temperatures[M].Berlin:Springer-Verlag,1987.,1987. |
[19] | 林明通,蒋丹宇,朱国强,施剑林.空洞蠕变的理论模型[J].硅酸盐通报,2001(05):16-21,46. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%